General
Property | Temperature | Value | Comment |
---|---|---|---|
Relative density | 23.0 °C | 1.27 [-] Show Supplier Material materials with Relative density of 1.27 [-] | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 3.8 GPa Show Supplier Material materials with Elastic modulus of 3.8 GPa | ASTM D 638 | 5 mm/min |
Elongation | 23.0 °C | 4.1 % Show Supplier Material materials with Elongation of 4.1 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 3.6 GPa Show Supplier Material materials with Flexural modulus of 3.6 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Flexural strength | 23.0 °C | 110 MPa Show Supplier Material materials with Flexural strength of 110 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Impact strength, Izod notched | 23.0 °C | 170 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 170 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 170 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 170 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 700 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 700 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 60 MPa Show Supplier Material materials with Tensile strength of 60 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 119 - 125 °C Show Supplier Material materials with Heat deflection temperature of 119 - 125 °C | ||
Heat deflection temperature, 0.45 MPa | 125 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 125 °C | ASTM D 648 | 3.2 mm | |
Heat deflection temperature, 1.80 MPa | 119 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 119 °C | ASTM D 648 | 1.82 MPa, 3.2 mm | |
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=102822332- - <br> UL Recognized, 94HB Flame Class Rating: 0.5mm UL 94 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant | 23.0 °C | 3.05 [-] Show Supplier Material materials with Dielectric constant of 3.05 [-] | SABIC method | 1.9 GHz |
Dielectric constant, 1GHz | 23.0 °C | 3.05 [-] Show Supplier Material materials with Dielectric constant, 1GHz of 3.05 [-] | SABIC method | 1.1 GHz |
Dielectric constant, 5GHz | 23.0 °C | 3.03 [-] Show Supplier Material materials with Dielectric constant, 5GHz of 3.03 [-] | SABIC method |
Dissipation factor | 23.0 °C | 0.01 [-] Show Supplier Material materials with Dissipation factor of 0.01 [-] | SABIC method |
Dissipation factor, 1GHz | 23.0 °C | 0.01 [-] Show Supplier Material materials with Dissipation factor, 1GHz of 0.01 [-] | SABIC method | |
Dissipation factor, 5GHz | 23.0 °C | 0.01 [-] Show Supplier Material materials with Dissipation factor, 5GHz of 0.01 [-] | SABIC method |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 29 g/10min Show Supplier Material materials with Melt mass-flow rate of 29 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Shrinkage | 23.0 °C | 0.3 % Show Supplier Material materials with Shrinkage of 0.3 % | SABIC method | 3.2 mm |
Shrinkage, transverse | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage, transverse of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Antenna | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 110°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |