General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.15 g/cm³ Show Supplier Material materials with Density of 1.15 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.02 % Show Supplier Material materials with Moisture absorption of 0.02 % | ASTM D 570 | (23°C/50% RH/24 hrs) |
Water absorption | 23.0 °C | 0.1 % Show Supplier Material materials with Water absorption of 0.1 % | ASTM D 570 | (23°C/24hrs) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 16 GPa Show Supplier Material materials with Elastic modulus of 16 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 0.9 % Show Supplier Material materials with Elongation of 0.9 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 12 GPa Show Supplier Material materials with Flexural modulus of 12 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 125 MPa Show Supplier Material materials with Flexural strength of 125 MPa | ISO 178 | 2 mm/min |
Impact strength, Izod notched | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 5 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 45 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 45 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched | 23.0 °C | 12 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 12 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 200 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 200 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 90 MPa Show Supplier Material materials with Tensile strength of 90 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 8.9E-6 1/K Show Supplier Material materials with Coefficient of thermal expansion of 8.9E-6 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 6.5E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 6.5E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Heat deflection temperature | 135 - 141 °C Show Supplier Material materials with Heat deflection temperature of 135 - 141 °C | ||||
Heat deflection temperature, 0.45 MPa | 141 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 141 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 135 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 135 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101283904- - <br> UL Recognized, 94HB Flame Class Rating: 1.5mm UL 94 <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=103093725- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100 - 1000000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100 - 1000000 Ω | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Personal Computing, Document Handling | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |