Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 10 GPa Show Supplier Material materials with Elastic modulus of 10 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 2 % Show Supplier Material materials with Elongation of 2 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 8.2 GPa Show Supplier Material materials with Flexural modulus of 8.2 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 210 MPa Show Supplier Material materials with Flexural strength of 210 MPa | ISO 178 | break, 2 mm/min |
Tensile strength | 23.0 °C | 160 MPa Show Supplier Material materials with Tensile strength of 160 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 215 °C Show Supplier Material materials with Heat deflection temperature of 215 °C | ||
Heat deflection temperature, 1.80 MPa | 215 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 215 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |
Relative temperature index, electrical | 105 °C Show Supplier Material materials with Relative temperature index, electrical of 105 °C | UL 746B | |
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |
Relative temperature index, mechanical strength | 105 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C | UL 746B | |
Flammability | UL Recognized, 94-5VA Flame Class Rating: ≥1.5mm UL 94 <br> Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221121- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 4 V Show Supplier Material materials with Comparative tracking index of 4 V | UL 746A | (UL) {PLC} |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 3 |
High Volt Arc Track Rate | 23.0 °C | 3 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 3 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 0 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.2 % Show Supplier Material materials with Shrinkage of 0.2 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Heavy Vehicles, Aircraft Seating, Air Cabin Interiors, Meter Gas | |
Availability | Europe,Asia,Americas | |
Processing methods | Mold Temperature: 140 to 180.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |