General
Property | Temperature | Value | Comment |
---|---|---|---|
Relative density | 23.0 °C | 1.2 [-] Show Supplier Material materials with Relative density of 1.2 [-] | ASTM D 792 | |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2 GPa Show Supplier Material materials with Elastic modulus of 2 GPa | ASTM D 638 | 5 mm/min |
Elongation | 23.0 °C | 94 % Show Supplier Material materials with Elongation of 94 % | ASTM D 638 | brk, Type I, 50 mm/min |
Flexural modulus | 23.0 °C | 2.4 GPa Show Supplier Material materials with Flexural modulus of 2.4 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Flexural strength | 23.0 °C | 88 MPa Show Supplier Material materials with Flexural strength of 88 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Impact strength, Charpy notched | 23.0 °C | 35 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 35 kJ/m² | ISO 179/1eA | 80*10*4mm, Cut, 23°C |
Impact strength, Izod notched | 23.0 °C | 45 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 45 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 630 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 630 J/m | ASTM D 256 |
Instrumented Impact, at Peak | 23.0 °C | 56 J Show Supplier Material materials with Instrumented Impact, at Peak of 56 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 62 MPa Show Supplier Material materials with Tensile strength of 62 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 7E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 7E-5 1/K | ASTM E 831 | 23°C to 80°C | ||
Heat deflection temperature | 127 °C Show Supplier Material materials with Heat deflection temperature of 127 °C | ||||
Heat deflection temperature, 1.80 MPa | 127 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 127 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Relative temperature index, electrical | 100 °C Show Supplier Material materials with Relative temperature index, electrical of 100 °C | UL 746B | |||
Relative temperature index, mechanical impact | 100 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 100 °C | UL 746B | |||
Relative temperature index, mechanical strength | 100 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 100 °C | UL 746B | |||
Thermal conductivity | 23.0 °C | 0.2 W/(m·K) Show Supplier Material materials with Thermal conductivity of 0.2 W/(m·K) | ISO 8302 | ||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221024- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=100726470- - <br> UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 3 V Show Supplier Material materials with Comparative tracking index of 3 V | UL 746A | (UL) {PLC} |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 2 |
High Volt Arc Track Rate | 23.0 °C | 2 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 2 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 18.2 g/10min Show Supplier Material materials with Melt mass-flow rate of 18.2 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Melt volume-flow rate | 15 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 15 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg | |
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Wireless Communications, Personal Computing, Semiconductor, Respiratory, Data Transfer, Data Management, Document Handling, Industrial Material Handling | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |