General
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.32 [-] Show Supplier Material materials with Coefficient of friction of 0.32 [-] | ||
Coefficient of friction, kinetic | 0.32 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.32 [-] | ASTM D 3702 Modified: Manual | |
Density | 23.0 °C | 1.31 g/cm³ Show Supplier Material materials with Density of 1.31 g/cm³ | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2.2 GPa Show Supplier Material materials with Elastic modulus of 2.2 GPa | ASTM D 638 | 5 mm/min |
Elongation | 23.0 °C | 33 % Show Supplier Material materials with Elongation of 33 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 2.3 GPa Show Supplier Material materials with Flexural modulus of 2.3 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Flexural strength | 23.0 °C | 86 MPa Show Supplier Material materials with Flexural strength of 86 MPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Impact strength, Izod notched | 23.0 °C | 119 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 119 kJ/m² | ASTM D 256 | notched, 23°C |
Tensile strength | 23.0 °C | 56 MPa Show Supplier Material materials with Tensile strength of 56 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 7.1E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 7.1E-5 1/K | ASTM D 696 | -30°C to 30°C |
Coefficient of thermal expansion, transverse | 23.0 °C | 7.5E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 7.5E-5 1/K | ASTM D 696 | -30°C to 30°C |
Heat deflection temperature | 130 - 141 °C Show Supplier Material materials with Heat deflection temperature of 130 - 141 °C | ||
Heat deflection temperature, 0.45 MPa | 141 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 141 °C | ASTM D 648 | 3.2 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 130 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 130 °C | ASTM D 648 | 3.2mm, unannealed |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.6 % Show Supplier Material materials with Shrinkage of 0.6 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | ATM/Ticket Machine, Document Handling, Personal Computing | |
Availability | Europe,Americas | |
Processing methods | Screw Speed: 30 to 60.0rpm | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |