Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 3.4 GPa Show Supplier Material materials with Elastic modulus of 3.4 GPa | ASTM D 638 | 5 mm/min |
Elongation | 23.0 °C | 60 % Show Supplier Material materials with Elongation of 60 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 3.4 GPa Show Supplier Material materials with Flexural modulus of 3.4 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Flexural strength | 23.0 °C | 165 MPa Show Supplier Material materials with Flexural strength of 165 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Impact strength, Izod notched | 23.0 °C | 26 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 26 kJ/m² | ASTM D 256 | notched, 23°C |
Tensile strength | 23.0 °C | 82 MPa Show Supplier Material materials with Tensile strength of 82 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 4.86E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 4.86E-5 1/K | ASTM E 831 | -40°C to 40°C |
Coefficient of thermal expansion, transverse | 23.0 °C | 4.86E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 4.86E-5 1/K | ASTM E 831 | -40°C to 40°C |
Heat deflection temperature | 165 °C Show Supplier Material materials with Heat deflection temperature of 165 °C | ||
Heat deflection temperature, 1.80 MPa | 165 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 165 °C | ASTM D 648 | 6.4 mm, unannealed | |
Vicat softening temperature | 181 °C Show Supplier Material materials with Vicat softening temperature of 181 °C | ASTM D 1525 | Rate B/50 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.6 % Show Supplier Material materials with Shrinkage of 0.6 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Food Container, Personal Computing | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Time (Cumulative): 24hrs | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |