General
Property | Temperature | Value | Comment |
---|---|---|---|
Relative density | 23.0 °C | 1.36 [-] Show Supplier Material materials with Relative density of 1.36 [-] | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 3.7 GPa Show Supplier Material materials with Elastic modulus of 3.7 GPa | ASTM D 638 | 5 mm/min |
Elongation | 23.0 °C | 70 % Show Supplier Material materials with Elongation of 70 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 3.7 GPa Show Supplier Material materials with Flexural modulus of 3.7 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Flexural strength | 23.0 °C | 165 MPa Show Supplier Material materials with Flexural strength of 165 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Tensile strength | 23.0 °C | 110 MPa Show Supplier Material materials with Tensile strength of 110 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Thermal
Property | Value | Comment |
---|---|---|
Heat deflection temperature | 198 °C Show Supplier Material materials with Heat deflection temperature of 198 °C | |
Heat deflection temperature, 1.80 MPa | 198 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 198 °C | ASTM D 648 | 6.4 mm, unannealed |
Relative temperature index, electrical | 170 °C Show Supplier Material materials with Relative temperature index, electrical of 170 °C | UL 746B |
Relative temperature index, mechanical impact | 170 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 170 °C | UL 746B |
Relative temperature index, mechanical strength | 170 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 170 °C | UL 746B |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 4 V Show Supplier Material materials with Comparative tracking index of 4 V | UL 746A | (UL) {PLC} |
High Amp Arc Ignition | 23.0 °C | 3 mm Show Supplier Material materials with High Amp Arc Ignition of 3 mm | UL 746A | surface {PLC} |
High Volt Arc Track Rate | 23.0 °C | 2 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1 mm Show Supplier Material materials with Hot-Wire Ignition of 1 mm | UL 746A | (PLC) |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 16 g/10min Show Supplier Material materials with Melt mass-flow rate of 16 g/10min | ASTM D 1238 | 337°C/6.6 kgf | |
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Microwave Oven, Servingware, Small Appliance, Airline Service, Aerospace, Air Cabin Interiors, Heavy Vehicles | |
Availability | Europe,Americas | |
Processing methods | Drying Time: 4 to 6.0hrs | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |