General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.19 g/cm³ Show Supplier Material materials with Density of 1.19 g/cm³ | ISO 1183 |
Limiting oxygen index | 23.0 °C | 35 % Show Supplier Material materials with Limiting oxygen index of 35 % | |
Moisture absorption | 23.0 °C | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.18 [-] Show Supplier Material materials with Relative density of 1.18 [-] | ASTM D 792 |
Water absorption | 23.0 °C | 0.35 % Show Supplier Material materials with Water absorption of 0.35 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elastic modulus | 23.0 °C | 2.1 GPa Show Supplier Material materials with Elastic modulus of 2.1 GPa | ISO 527 | 1 mm/min | ||
Elongation | 23.0 °C | 125 % Show Supplier Material materials with Elongation of 125 % | ISO 527 | break, 50 mm/min | ||
Flexural modulus | 23.0 °C | 2.2 GPa Show Supplier Material materials with Flexural modulus of 2.2 GPa | ISO 178 | 2 mm/min | ||
Flexural strength | 23.0 °C | 85 MPa Show Supplier Material materials with Flexural strength of 85 MPa | ISO 178 | yield, 2 mm/min | ||
Hardness, Ball Indentation | 23.0 °C | 90 MPa Show Supplier Material materials with Hardness, Ball Indentation of 90 MPa | ISO 2039-1 | H358/30 | ||
Impact strength, Charpy notched | 23.0 °C | 60 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 60 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*3 sp=62mm, -30°C | ||
Impact strength, Izod notched | 23.0 °C | 80 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 80 kJ/m² | ISO 180/4A | notched 63.5*12.7*3.2, 23°C, | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 801 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 801 J/m | ASTM D 256 | notched, 23°C | ||
Instrumented Impact, Total Energy | 23.0 °C | 52 J Show Supplier Material materials with Instrumented Impact, Total Energy of 52 J | ASTM D 3763 | 23°C | ||
Tensile strength | 23.0 °C | 60 MPa Show Supplier Material materials with Tensile strength of 60 MPa | ISO 527 | break, 50 mm/min | ||
Impact strength, Charpy unnotched | ISO 179/1eU | Unnotch Edgew 80*10*3 sp=62mm, 23°C | ||||
Impact strength, Izod unnotched | ISO 180/1U | 80*10*3, 23°C |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 125°C +/- 2°C | |||
Coefficient of thermal expansion | 23.0 °C | 7.2E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 7.2E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 7.7E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 7.7E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Heat deflection temperature | 124 - 135 °C Show Supplier Material materials with Heat deflection temperature of 124 - 135 °C | ||||
Heat deflection temperature, 0.45 MPa | 135 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 135 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 124 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 124 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Relative temperature index, electrical | 125 °C Show Supplier Material materials with Relative temperature index, electrical of 125 °C | UL 746B | |||
Relative temperature index, mechanical impact | 115 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 115 °C | UL 746B | |||
Relative temperature index, mechanical strength | 120 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 120 °C | UL 746B | |||
Vicat softening temperature | 142 °C Show Supplier Material materials with Vicat softening temperature of 142 °C | ISO 306 | Rate B/120 | |||
Flammability | Glow Wire Ignitability Temperature, 1.0 mm: 825°C IEC 60695-2-13 <br> Glow Wire Flammability Index 960°C, passes at: 1mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 1mm IEC 60695-2-12 <br> UL Recognized, 94V-1 Flame Class Rating: 0.8mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: 1.49mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: 2.99mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 225 V Show Supplier Material materials with Comparative tracking index of 225 V | IEC 60112 | |
Dielectric strength | 23.0 °C | 16 kV/mm Show Supplier Material materials with Dielectric strength of 16 kV/mm | IEC 60243-1 | in oil, 3.2 mm, |
Dissipation factor, 1MHz | 23.0 °C | 8.5E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 8.5E-3 [-] | IEC 60250 |
Dissipation factor, 50Hz | 23.0 °C | 1E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 1E-3 [-] | IEC 60250 | 50/60 Hz |
High Amp Arc Ignition | 23.0 °C | 0 mm Show Supplier Material materials with High Amp Arc Ignition of 0 mm | UL 746A | surface {PLC} |
Hot-Wire Ignition | 23.0 °C | 1 mm Show Supplier Material materials with Hot-Wire Ignition of 1 mm | UL 746A | (PLC) |
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | >, IEC 60093 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | >, IEC 60093 | |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 10 g/10min Show Supplier Material materials with Melt mass-flow rate of 10 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Melt volume-flow rate | 9 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 9 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg | |
Shrinkage | 23.0 °C | 0.4 % Show Supplier Material materials with Shrinkage of 0.4 % | SABIC method | 3.2 mm |
Shrinkage, transverse | 23.0 °C | 0.4 % Show Supplier Material materials with Shrinkage, transverse of 0.4 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Data Management, Enclosures, Electronic Components, EV Infrastructure, Photovoltaic Components, Power Manangement | |
Availability | Europe,Asia | |
Processing methods | Rear - Zone 1 Temperature: 270 to 295.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |