General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.68 g/cm³ Show Supplier Material materials with Density of 1.68 g/cm³ | ASTM D 792 |
Water absorption | 23.0 °C | 0.06 % Show Supplier Material materials with Water absorption of 0.06 % | ASTM D 570 | (23°C/24hrs) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 2.5 % Show Supplier Material materials with Elongation of 2.5 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 9.7 GPa Show Supplier Material materials with Flexural modulus of 9.7 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Flexural strength | 23.0 °C | 165 MPa Show Supplier Material materials with Flexural strength of 165 MPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Impact strength, Izod notched | 23.0 °C | 64 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 64 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 64 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 64 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 370 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 370 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 121 MPa Show Supplier Material materials with Tensile strength of 121 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 204 °C Show Supplier Material materials with Heat deflection temperature of 204 °C | ||
Heat deflection temperature, 1.80 MPa | 204 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 204 °C | ASTM D 648 | 3.2mm, unannealed | |
Flammability | UL Recognized, 94V-0 Flame Class Rating: 0.73mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101358191- - |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.4 % Show Supplier Material materials with Shrinkage of 0.4 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Electrical, Document Handling, Auto Electrical, Circuit Protection | |
Availability | Europe,Asia,Americas | |
Processing methods | Melt Temperature: 245 to 260.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |