General
Property | Temperature | Value | Comment |
---|---|---|---|
Relative density | 23.0 °C | 1.03 [-] Show Supplier Material materials with Relative density of 1.03 [-] | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 0.7 GPa Show Supplier Material materials with Elastic modulus of 0.7 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 20 % Show Supplier Material materials with Elongation of 20 % | ISO 527 | yield, 50 mm/min |
Flexural modulus | 23.0 °C | 0.8 GPa Show Supplier Material materials with Flexural modulus of 0.8 GPa | ISO 178 |
Hardness, Shore D | 23.0 °C | 63 [-] Show Supplier Material materials with Hardness, Shore D of 63 [-] | ASTM D 2240 | 10S reading |
Impact strength, Izod notched | 23.0 °C | 37 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 37 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 170 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 170 J/m | ASTM D 256 |
Tensile strength | 23.0 °C | 25 MPa Show Supplier Material materials with Tensile strength of 25 MPa | ISO 527 | break, 50 mm/min |
Thermal
Property | Value | Comment |
---|---|---|
Heat deflection temperature | 66 - 82 °C Show Supplier Material materials with Heat deflection temperature of 66 - 82 °C | |
Heat deflection temperature, 0.45 MPa | 82 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 82 °C | ASTM D 648 | 3.2 mm, unannealed |
Heat deflection temperature, 1.80 MPa | 66 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 66 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 1GHz | 23.0 °C | 2.47 [-] Show Supplier Material materials with Dielectric constant, 1GHz of 2.47 [-] | ASTM D 150 |
Dissipation factor, 1GHz | 23.0 °C | 3.2E-3 [-] Show Supplier Material materials with Dissipation factor, 1GHz of 3.2E-3 [-] | ASTM D 150 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Melt mass-flow rate | 33 g/10min Show Supplier Material materials with Melt mass-flow rate of 33 g/10min | ASTM D 1238 | 280°C/5.0 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Airbag, Auto Electrical, Wire & cable | |
Availability | Europe,Asia,Americas | |
Processing methods | Water Bath Temperature: 15 to 30.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |