General
Property | Temperature | Value | Comment |
---|---|---|---|
Relative density | 23.0 °C | 1.26 [-] Show Supplier Material materials with Relative density of 1.26 [-] | ASTM D 792 | |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 3 GPa Show Supplier Material materials with Elastic modulus of 3 GPa | ASTM D 638 | 5 mm/min |
Elongation | 23.0 °C | 10 % Show Supplier Material materials with Elongation of 10 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 3.1 GPa Show Supplier Material materials with Flexural modulus of 3.1 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Flexural strength | 23.0 °C | 107 MPa Show Supplier Material materials with Flexural strength of 107 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Impact strength, Izod notched | 23.0 °C | 214 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 214 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 214 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 214 J/m | ASTM D 256 |
Tensile strength | 23.0 °C | 66 MPa Show Supplier Material materials with Tensile strength of 66 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Thermal
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 34 g/10min Show Supplier Material materials with Melt mass-flow rate of 34 g/10min | ASTM D 1238 | 295°C/6.6 kgf | |
Shrinkage | 23.0 °C | 0.4 % Show Supplier Material materials with Shrinkage of 0.4 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Personal Computing, Wireless Communications | |
Availability | Asia,Americas | |
Processing methods | Shot to Cylinder Size: 50 to 70.0% | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |