General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.7 g/cm³ Show Supplier Material materials with Density of 1.7 g/cm³ | ISO 1183 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 1.8 % Show Supplier Material materials with Elongation of 1.8 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 19 GPa Show Supplier Material materials with Flexural modulus of 19 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 335 MPa Show Supplier Material materials with Flexural strength of 335 MPa | ISO 178 | break, 2 mm/min |
Impact strength, Izod notched | 23.0 °C | 14 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 14 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod unnotched | 23.0 °C | 65 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 65 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Tensile strength | 23.0 °C | 235 MPa Show Supplier Material materials with Tensile strength of 235 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 6E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 6E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Heat deflection temperature | 220 °C Show Supplier Material materials with Heat deflection temperature of 220 °C | ||||
Heat deflection temperature, 1.80 MPa | 220 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 220 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Flammability | UL Compliant, 94HB Flame Class Rating: 0.8mm UL 94 by SABIC-IP |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.1 % Show Supplier Material materials with Shrinkage of 0.1 % | SABIC method |
Technological properties
Property | ||
---|---|---|
Application areas | Wiring Devices, Washing Machine, Electronic Components, Dishwasher | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |