General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.57 g/cm³ Show Supplier Material materials with Density of 1.57 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.97 % Show Supplier Material materials with Moisture absorption of 0.97 % | ISO 62 | (23°C / 50% RH) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 14 GPa Show Supplier Material materials with Elastic modulus of 14 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 3 % Show Supplier Material materials with Elongation of 3 % | ISO 527 | break |
Flexural modulus | 23.0 °C | 13.3 GPa Show Supplier Material materials with Flexural modulus of 13.3 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 320 MPa Show Supplier Material materials with Flexural strength of 320 MPa | ISO 178 | break, 2 mm/min |
Impact strength, Izod notched | 23.0 °C | 16 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 16 kJ/m² | ISO 180/1A | notched 80*10*4 |
Impact strength, Izod unnotched | 23.0 °C | 94 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 94 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Tensile strength | 23.0 °C | 241 MPa Show Supplier Material materials with Tensile strength of 241 MPa | ISO 527 | break |
Thermal
Rheological Properties
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Middle - Zone 2 Temperature: 250 to 280.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |