General
Property | Temperature | Value | Comment |
---|---|---|---|
Relative density | 23.0 °C | 1.18 [-] Show Supplier Material materials with Relative density of 1.18 [-] | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 50 % Show Supplier Material materials with Elongation of 50 % | ASTM D 638 | break |
Flexural modulus | 23.0 °C | 2.7 GPa Show Supplier Material materials with Flexural modulus of 2.7 GPa | ASTM D 790 |
Flexural strength | 23.0 °C | 103 MPa Show Supplier Material materials with Flexural strength of 103 MPa | ASTM D 790 |
Tensile strength | 23.0 °C | 66 MPa Show Supplier Material materials with Tensile strength of 66 MPa | ASTM D 638 | yield |
Thermal
Property | Value | Comment | |
---|---|---|---|
Relative temperature index, electrical | 85 °C Show Supplier Material materials with Relative temperature index, electrical of 85 °C | UL 746B | |
Relative temperature index, mechanical impact | 85 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 85 °C | UL 746B | |
Relative temperature index, mechanical strength | 85 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 85 °C | UL 746B | |
Flammability | UL Recognized, 94HB Flame Class Rating: ≥0.7mm UL 94 <br> UL Recognized, 94V-1 Flame Class Rating: ≥1.2mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: ≥3.4mm UL 94 <br> UL Recognized, 94-5VB Flame Class Rating: ≥2.0mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=104340779- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 2 V Show Supplier Material materials with Comparative tracking index of 2 V | UL 746A | (UL) {PLC} |
Dielectric constant, 1MHz | 23.0 °C | 2.7 [-] Show Supplier Material materials with Dielectric constant, 1MHz of 2.7 [-] | IEC 60250 |
Dielectric constant, 60Hz | 23.0 °C | 2.8 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.8 [-] | IEC 60250 |
Dielectric strength | 23.0 °C | 430 kV/mm Show Supplier Material materials with Dielectric strength of 430 kV/mm | IEC 60243-1 | in oil, 3.2 mm, |
Dissipation factor, 1MHz | 23.0 °C | 8E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 8E-3 [-] | IEC 60250 |
Dissipation factor, 50Hz | 23.0 °C | 4E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 4E-3 [-] | IEC 60250 | 50/60 Hz |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 2 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 2 |
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | ASTM D 257 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 17 g/10min Show Supplier Material materials with Melt mass-flow rate of 17 g/10min | ASTM D 1238 | 260°C/2.16 kgf | |
Shrinkage | 23.0 °C | 0.4 % Show Supplier Material materials with Shrinkage of 0.4 % | SABIC method |
Shrinkage, transverse | 23.0 °C | 0.4 % Show Supplier Material materials with Shrinkage, transverse of 0.4 % | SABIC method |
Technological properties
Property | ||
---|---|---|
Application areas | Medical Facility Infrastructure | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80 to 90.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |