General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.24 g/cm³ Show Supplier Material materials with Density of 1.24 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.05 % Show Supplier Material materials with Moisture absorption of 0.05 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.24 [-] Show Supplier Material materials with Relative density of 1.24 [-] | ASTM D 792 | |
Water absorption | 23.0 °C | 0.12 % Show Supplier Material materials with Water absorption of 0.12 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elastic modulus | 23.0 °C | 2.2 GPa Show Supplier Material materials with Elastic modulus of 2.2 GPa | ISO 527 | 1 mm/min | ||
Elongation | 23.0 °C | 100 % Show Supplier Material materials with Elongation of 100 % | ISO 527 | break, 50 mm/min | ||
Flexural modulus | 23.0 °C | 2.2 GPa Show Supplier Material materials with Flexural modulus of 2.2 GPa | ISO 178 | 2 mm/min | ||
Flexural strength | 23.0 °C | 86 MPa Show Supplier Material materials with Flexural strength of 86 MPa | ISO 178 | yield, 2 mm/min | ||
Impact strength, Charpy notched | 23.0 °C | 50 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 50 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*3 sp=62mm, -30°C | ||
Impact strength, Izod notched | 23.0 °C | 50 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 50 kJ/m² | ISO 180/1A | notched 80*10*3, -30°C | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 550 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 550 J/m | ASTM D 256 | ||
Tensile strength | 23.0 °C | 58 MPa Show Supplier Material materials with Tensile strength of 58 MPa | ISO 527 | break, 50 mm/min | ||
Impact strength, Charpy unnotched | ISO 179/1eU | Unnotch Edgew 80*10*3 sp=62mm, 23°C | ||||
Impact strength, Izod unnotched | ISO 180/1U | unnotched 80*10*3, 23°C, |
Thermal
Property | Value | Comment |
---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 125°C +/- 2°C |
Heat deflection temperature | 126 - 139 °C Show Supplier Material materials with Heat deflection temperature of 126 - 139 °C | |
Heat deflection temperature, 0.45 MPa | 139 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 139 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm |
Heat deflection temperature, 1.80 MPa | 126 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 126 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm |
Vicat softening temperature | 147 °C Show Supplier Material materials with Vicat softening temperature of 147 °C | ISO 306 | Rate B/120 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 250 V Show Supplier Material materials with Comparative tracking index of 250 V | IEC 60112 | |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 8 g/10min Show Supplier Material materials with Melt mass-flow rate of 8 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Melt volume-flow rate | 7 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 7 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg | |
Shrinkage | 23.0 °C | 0.4 % Show Supplier Material materials with Shrinkage of 0.4 % | SABIC method | 3.2 mm |
Shrinkage, transverse | 23.0 °C | 0.4 % Show Supplier Material materials with Shrinkage, transverse of 0.4 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Photovoltaic Components, Rail Cabin Interiors, Non-LED Lighting, Electronic Components, Air Conditioning | |
Availability | Europe,Asia,Americas | |
Processing methods | Middle - Zone 2 Temperature: 280 to 305.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |