General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.19 g/cm³ Show Supplier Material materials with Density of 1.19 g/cm³ | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 78 % Show Supplier Material materials with Elongation of 78 % | ASTM D 638 | brk, Type I, 50 mm/min |
Flexural modulus | 23.0 °C | 2.3 GPa Show Supplier Material materials with Flexural modulus of 2.3 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Hardness, Rockwell R | 23.0 °C | 127 [-] Show Supplier Material materials with Hardness, Rockwell R of 127 [-] | ASTM D 785 |
Impact strength, Izod notched | 23.0 °C | 373 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 373 kJ/m² | ASTM D 256 | notched, 23°C |
Tensile strength | 23.0 °C | 65 MPa Show Supplier Material materials with Tensile strength of 65 MPa | ASTM D 638 | yld, Type I, 50 mm/min |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 8.1E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 8.1E-5 1/K | ASTM E 831 | -40°C to 95°C |
Heat deflection temperature | 148 °C Show Supplier Material materials with Heat deflection temperature of 148 °C | ||
Heat deflection temperature, 1.80 MPa | 148 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 148 °C | ASTM D 648 | 3.2mm, unannealed | |
Thermal conductivity | 23.0 °C | 0.21 W/(m·K) Show Supplier Material materials with Thermal conductivity of 0.21 W/(m·K) | ASTM C177 |
Electrical
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.9 % Show Supplier Material materials with Shrinkage of 0.9 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Wireless Communications, Respiratory, Rear/Signal Lighting, Recreational Vehicle, Overhead, Microwave Oven, LED Lighting, Medical Device, Non-LED Lighting, Motorcycle, Data Transfer, Displays, Dishwasher, Auto Aftermarket, Enclosure/Housing/Cover, Electronic Components, Forward Lighting, Fog Lamp | |
Availability | Europe,Asia,Americas | |
Processing methods | Nozzle Temperature: 345 to 365.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |