Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.2 g/cm³ Show Supplier Material materials with Density of 1.2 g/cm³ | ISO 1183 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 7 % Show Supplier Material materials with Elongation of 7 % | ISO 527 | yield, 50 mm/min |
Flexural modulus | 23.0 °C | 2.3 GPa Show Supplier Material materials with Flexural modulus of 2.3 GPa | ISO 178 | 2 mm/min |
Hardness, Rockwell R | 23.0 °C | 127 [-] Show Supplier Material materials with Hardness, Rockwell R of 127 [-] | ISO 2039-2 |
Impact strength, Izod notched | 23.0 °C | 11 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 11 kJ/m² | ISO 180/1A | notched 80*10*3, -30°C |
Tensile strength | 23.0 °C | 70 MPa Show Supplier Material materials with Tensile strength of 70 MPa | ISO 527 | yield, 50 mm/min |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 8E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 8E-5 1/K | ISO 11359-2 | 23°C to 80°C |
Heat deflection temperature | 151 °C Show Supplier Material materials with Heat deflection temperature of 151 °C | ||
Heat deflection temperature, 1.80 MPa | 151 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 151 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Thermal conductivity | 23.0 °C | 0.21 W/(m·K) Show Supplier Material materials with Thermal conductivity of 0.21 W/(m·K) | ISO 8302 |
Electrical
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.8 % Show Supplier Material materials with Shrinkage of 0.8 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Wireless Communications, Respiratory, Rear/Signal Lighting, Recreational Vehicle, Overhead, Microwave Oven, LED Lighting, Medical Device, Non-LED Lighting, Motorcycle, Data Transfer, Displays, Dishwasher, Auto Aftermarket, Enclosure/Housing/Cover, Electronic Components, Forward Lighting, Fog Lamp | |
Availability | Europe,Asia,Americas | |
Processing methods | Rear - Zone 1 Temperature: 300 to 320.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |