General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.09 g/cm³ Show Supplier Material materials with Density of 1.09 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.05 % Show Supplier Material materials with Moisture absorption of 0.05 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.09 [-] Show Supplier Material materials with Relative density of 1.09 [-] | ASTM D 792 | |
Water absorption | 23.0 °C | 0.25 % Show Supplier Material materials with Water absorption of 0.25 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2.2 GPa Show Supplier Material materials with Elastic modulus of 2.2 GPa | ASTM D 638 | 5 mm/min |
Elongation | 23.0 °C | 12 % Show Supplier Material materials with Elongation of 12 % | ASTM D 638 | brk, Type I, 50 mm/min |
Flexural modulus | 23.0 °C | 2.5 GPa Show Supplier Material materials with Flexural modulus of 2.5 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Flexural strength | 23.0 °C | 100 MPa Show Supplier Material materials with Flexural strength of 100 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Impact strength, Izod notched | 23.0 °C | 227 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 227 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 69 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 69 J/m | ASTM D 256 | notched, -30°C |
Instrumented Impact, Total Energy | 23.0 °C | 53 J Show Supplier Material materials with Instrumented Impact, Total Energy of 53 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 59 MPa Show Supplier Material materials with Tensile strength of 59 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball pressure temperature | 145 °C Show Supplier Material materials with Ball pressure temperature of 145 °C | IEC 60695-10-2 | approximate maximum | |||
Coefficient of thermal expansion | 23.0 °C | 8E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 8E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 8E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 8E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 800 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 800 °C | IEC 60695-2-13 | 3.0 mm | |||
Heat deflection temperature | 139 °C Show Supplier Material materials with Heat deflection temperature of 139 °C | ||||
Heat deflection temperature, 1.80 MPa | 139 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 139 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 105 °C Show Supplier Material materials with Relative temperature index, electrical of 105 °C | UL 746B | |||
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |||
Relative temperature index, mechanical strength | 105 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C | UL 746B | |||
Vicat softening temperature | 162 °C Show Supplier Material materials with Vicat softening temperature of 162 °C | ISO 306 | Rate B/120 | |||
Flammability | UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 <br> Glow Wire Ignitability Temperature, 1.0 mm: 825°C IEC 60695-2-13 <br> Glow Wire Ignitability Temperature, 1.5 mm: 825°C IEC 60695-2-13 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=104159882- - <br> UV-light, water exposure/immersion: F1- UL 746C <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=104159890- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 3 V Show Supplier Material materials with Comparative tracking index of 3 V | UL 746A | (UL) {PLC} |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 1 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 0 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 20.1 g/10min Show Supplier Material materials with Melt mass-flow rate of 20.1 g/10min | ASTM D 1238 | 300°C/5.0 kgf | |
Melt volume-flow rate | 20 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 20 cm³/10min | ISO 1133 | MVR at 300°C/5.0 kg | |
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Wiring Devices, Respiratory, Security/Detection, Plumbing, Personal Computing, LED Lighting, Circuit Protection, Enclosures | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 110 to 120.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |