General
Property | Temperature | Value | Comment |
---|---|---|---|
Limiting oxygen index | 23.0 °C | 25 % Show Supplier Material materials with Limiting oxygen index of 25 % | |
Relative density | 23.0 °C | 1.03 [-] Show Supplier Material materials with Relative density of 1.03 [-] | ASTM D 792 |
Water absorption | 23.0 °C | 0.1 % Show Supplier Material materials with Water absorption of 0.1 % | ASTM D 570 | (23°C/48hrs) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 90 % Show Supplier Material materials with Elongation of 90 % | ISO 527 | break, 50 mm/min |
Flexural modulus | 23.0 °C | 0.7 GPa Show Supplier Material materials with Flexural modulus of 0.7 GPa | ISO 178 | 12.5 mm/min |
Hardness, Shore D | 23.0 °C | 56 [-] Show Supplier Material materials with Hardness, Shore D of 56 [-] | ISO 868 |
Tensile strength | 23.0 °C | 23 MPa Show Supplier Material materials with Tensile strength of 23 MPa | ISO 527 | break, 50 mm/min |
Thermal
Property | Value | Comment | |
---|---|---|---|
Brittleness temperature | -40 °C Show Supplier Material materials with Brittleness temperature of -40 °C | <, ASTM D 746 | |
Glow Wire Ignition Temperature | 750 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 750 °C | IEC 60695-2-13 | 3.0 mm | |
Heat deflection temperature | 85 °C Show Supplier Material materials with Heat deflection temperature of 85 °C | ||
Heat deflection temperature, 0.45 MPa | 85 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 85 °C | ASTM D 648 | 6.4 mm, unannealed | |
Vicat softening temperature | 102 °C Show Supplier Material materials with Vicat softening temperature of 102 °C | ISO 306 | Rate A/50 | |
Flammability | Glow Wire Flammability Index 960°C, passes at: 3mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3mm IEC 60695-2-12 <br> Smoke Density on 0.5mm plaque, Flame, Ds, max: 150- ASTM E 662 <br> Smoke Density on 0.5mm plaque, Non-flame, Ds, max: 75- ASTM E 662 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 600 V Show Supplier Material materials with Comparative tracking index of 600 V | IEC 60112 | |
Dielectric constant, 1MHz | 23.0 °C | 2.5 [-] Show Supplier Material materials with Dielectric constant, 1MHz of 2.5 [-] | IEC 60250 |
Dielectric constant, 60Hz | 23.0 °C | 2.6 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.6 [-] | IEC 60250 | 50/60 Hz |
Dielectric strength | 23.0 °C | 26 kV/mm Show Supplier Material materials with Dielectric strength of 26 kV/mm | IEC 60243-1 | in oil, 2.0mm |
Dissipation factor, 1MHz | 23.0 °C | 3.8E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 3.8E-3 [-] | IEC 60250 |
Dissipation factor, 50Hz | 23.0 °C | 0.02 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 0.02 [-] | IEC 60250 | 50/60 Hz |
Volume resistivity | 23.0 °C | 3.90E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 3.90E+16 Ω·cm | IEC 60093 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Melt mass-flow rate | 5.1 g/10min Show Supplier Material materials with Melt mass-flow rate of 5.1 g/10min | ASTM D 1238 | 250°C/10.0 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Data Transfer, Wire & cable | |
Availability | Americas | |
Processing methods | Screen Pack: 150 to 100.0- | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |