General
Property | Temperature | Value | Comment |
---|---|---|---|
Relative density | 23.0 °C | 1.01 [-] Show Supplier Material materials with Relative density of 1.01 [-] | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 175 % Show Supplier Material materials with Elongation of 175 % | ISO 527 | break, 50 mm/min |
Flexural modulus | 23.0 °C | 0.1 GPa Show Supplier Material materials with Flexural modulus of 0.1 GPa | ISO 178 | 12.5 mm/min |
Hardness, Shore A | 23.0 °C | 84 [-] Show Supplier Material materials with Hardness, Shore A of 84 [-] | ASTM D 2240 | 30S reading |
Tensile strength | 23.0 °C | 7 MPa Show Supplier Material materials with Tensile strength of 7 MPa | ISO 527 | break, 50 mm/min |
Thermal
Property | Value | Comment | |
---|---|---|---|
Brittleness temperature | -40 °C Show Supplier Material materials with Brittleness temperature of -40 °C | <, ASTM D 746 | |
Glow Wire Ignition Temperature | 750 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 750 °C | IEC 60695-2-13 | 3.0 mm | |
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101939210- - <br> UL Recognized, 94HB Flame Class Rating: ≥0.6mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥6mm UL 94 <br> Glow Wire Flammability Index 750°C, passes at: 3mm IEC 60695-2-12 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 0 V Show Supplier Material materials with Comparative tracking index of 0 V | UL 746A | (UL) {PLC} |
Volume resistivity | 23.0 °C | 7.10E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 7.10E+15 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 24 g/10min Show Supplier Material materials with Melt mass-flow rate of 24 g/10min | ASTM D 1238 | 210°C/5 kgf | |
Shrinkage | 23.0 °C | 0.95 % Show Supplier Material materials with Shrinkage of 0.95 % | ASTM D 955 | 24 hrs |
Shrinkage, transverse | 23.0 °C | 0.75 % Show Supplier Material materials with Shrinkage, transverse of 0.75 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Wire & cable | |
Availability | Asia,Americas | |
Processing methods | Drying Temperature: 60 to 80.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |