General
Property | Temperature | Value | Comment |
---|---|---|---|
Limiting oxygen index | 23.0 °C | 33.9 % Show Supplier Material materials with Limiting oxygen index of 33.9 % | |
Relative density | 23.0 °C | 1.16 [-] Show Supplier Material materials with Relative density of 1.16 [-] | ASTM D 792 |
Water absorption | 23.0 °C | 0.22 % Show Supplier Material materials with Water absorption of 0.22 % | ASTM D 570 | (23°C/Saturated) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 5 % Show Supplier Material materials with Elongation of 5 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 4 GPa Show Supplier Material materials with Flexural modulus of 4 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Flexural strength | 23.0 °C | 119 MPa Show Supplier Material materials with Flexural strength of 119 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Impact strength, Izod notched | 23.0 °C | 96 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 96 kJ/m² | ASTM D 256 | notched, 23°C |
Tensile strength | 23.0 °C | 74 MPa Show Supplier Material materials with Tensile strength of 74 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 131 °C Show Supplier Material materials with Heat deflection temperature of 131 °C | ||
Heat deflection temperature, 1.80 MPa | 131 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 131 °C | ASTM D 648 | 6.4 mm, unannealed | |
Relative temperature index, electrical | 110 °C Show Supplier Material materials with Relative temperature index, electrical of 110 °C | UL 746B | |
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |
Relative temperature index, mechanical strength | 110 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 110 °C | UL 746B | |
Vicat softening temperature | 147 °C Show Supplier Material materials with Vicat softening temperature of 147 °C | ASTM D 1525 | Rate B/50 | |
Flammability | UL Recognized, 94V-1 Flame Class Rating: ≥0.44mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: ≥2.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=228589- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=101825569- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 2 V Show Supplier Material materials with Comparative tracking index of 2 V | UL 746A | (UL) {PLC} |
Dielectric constant, 1MHz | 23.0 °C | 3 [-] Show Supplier Material materials with Dielectric constant, 1MHz of 3 [-] | ASTM D 150 |
Dielectric constant, 60Hz | 23.0 °C | 3 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 3 [-] | ASTM D 150 | 50/60 Hz |
Dissipation factor, 1MHz | 23.0 °C | 1.6E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 1.6E-3 [-] | ASTM D 150 | |
Dissipation factor, 50Hz | 23.0 °C | 1.7E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 1.7E-3 [-] | ASTM D 150 | 50/60 Hz |
High Amp Arc Ignition | 23.0 °C | 0.71 mm Show Supplier Material materials with High Amp Arc Ignition of 0.71 mm | ≥, UL 746A | PLC 2 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 0.71 mm Show Supplier Material materials with Hot-Wire Ignition of 0.71 mm | ≥, UL 746A | PLC 1 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.3 % Show Supplier Material materials with Shrinkage of 0.3 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Circuit Protection, Building Accessory, Auto Electrical, Battery Pack, Audio, Auto Aftermarket, Aerospace, Coffee Maker/Espresso Machine, Cladding/Roof, Document Handling, Displays, Dishwasher, Enclosures, Enclosure/Housing/Cover, Energy Management, Electronic Components, Humidity Control, Individual Equiptment, Eyeglasses, Freezer, Fixture Bath/Shower, Engine Component, EV/HEV Battery, Wiring Devices, Wireless Communications, Personal Computing, Monitoring and Imaging, Meter Gas, Medical Device, Respiratory, Plumbing, Photovoltaic Components, Power Manangement, Pump | |
Availability | Europe,Asia,Americas | |
Processing methods | Melt Temperature: 280 to 310.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |