NORYL™ N225X resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of 5VA at 3mm and V0 at 1.5mm along with a UL746C Outdoor Suitability rating of F1. NORYL N225X resin offers good dielectric strength and strong electrical performance in addition to low moisture absorption and dimensional stability, This material is an excellent candidate for both indoor and outdoor electrical applications.

This material data has been provided by Sabic.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Relative density

23.0 °C

1.11 [-]

Show Supplier Material materials with Relative density of 1.11 [-]

ASTM D 792 |

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

17 %

Show Supplier Material materials with Elongation of 17 %

ASTM D 638 | brk, Type I, 50 mm/min

Flexural modulus

23.0 °C

2.5 GPa

Show Supplier Material materials with Flexural modulus of 2.5 GPa

ASTM D 790 | 2.6 mm/min, 100 mm span

Flexural strength

23.0 °C

99 MPa

Show Supplier Material materials with Flexural strength of 99 MPa

ASTM D 790 | yld, 2.6 mm/min, 100 mm span

Impact strength, Izod notched

23.0 °C

186 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 186 kJ/m²

ASTM D 256 | notched, 23°C

Impact strength, Izod notched, ASTM

23.0 °C

96 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 96 J/m

ASTM D 256 | notched, -30°C

Instrumented Impact, at Peak

23.0 °C

39 J

Show Supplier Material materials with Instrumented Impact, at Peak of 39 J

ASTM D 3763 | 23°C

Tensile strength

23.0 °C

66 MPa

Show Supplier Material materials with Tensile strength of 66 MPa

ASTM D 638 | yld, Type I, 50 mm/min

Thermal

PropertyValueComment

Heat deflection temperature

99 - 109 °C

Show Supplier Material materials with Heat deflection temperature of 99 - 109 °C

Heat deflection temperature, 0.45 MPa

109 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 109 °C

ASTM D 648 | 6.4 mm, unannealed

Heat deflection temperature, 1.80 MPa

99 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 99 °C

ASTM D 648 | 6.4 mm, unannealed

Relative temperature index, electrical

95 °C

Show Supplier Material materials with Relative temperature index, electrical of 95 °C

UL 746B

Relative temperature index, mechanical impact

80 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C

UL 746B

Relative temperature index, mechanical strength

95 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 95 °C

UL 746B

Vicat softening temperature

128 °C

Show Supplier Material materials with Vicat softening temperature of 128 °C

ASTM D 1525 | Rate B/50

Flammability

UL Recognized, 94HB Flame Class Rating: ≥0.4mm UL 94 <br> Radiant Panel Listing: TRUE- UL Tested <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: ≥3mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221178- -

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

1 V

Show Supplier Material materials with Comparative tracking index of 1 V

UL 746A | (UL) {PLC}

Dielectric constant, 1MHz

23.0 °C

2.55 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 2.55 [-]

ASTM D 150

Dielectric constant, 60Hz

23.0 °C

2.69 [-]

Show Supplier Material materials with Dielectric constant, 60Hz of 2.69 [-]

ASTM D 150 | 50/60 Hz

Dielectric strength

23.0 °C

16.2 kV/mm

Show Supplier Material materials with Dielectric strength of 16.2 kV/mm

ASTM D 149 | in oil, 3.2 mm

Dissipation factor, 1MHz

23.0 °C

7E-3 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 7E-3 [-]

ASTM D 150

Dissipation factor, 50Hz

23.0 °C

0.01 [-]

Show Supplier Material materials with Dissipation factor, 50Hz of 0.01 [-]

ASTM D 150 | 50/60 Hz

High Amp Arc Ignition

23.0 °C

1.5 mm

Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm

≥, UL 746A | PLC 0

High Volt Arc Track Rate

23.0 °C

4 PLC Code

Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code

UL 746A | (PLC)

Hot-Wire Ignition

23.0 °C

6 mm

Show Supplier Material materials with Hot-Wire Ignition of 6 mm

≥, UL 746A | PLC 0

Sheet resistivity, ROA

23.0 °C

1.00E+14 Ω

Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+14 Ω

>, ASTM D 257

Volume resistivity

23.0 °C

2.80E+16 Ω·cm

Show Supplier Material materials with Volume resistivity of 2.80E+16 Ω·cm

ASTM D 257

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.5 %

Show Supplier Material materials with Shrinkage of 0.5 %

SABIC method | 3.2 mm

Shrinkage, transverse

23.0 °C

0.5 %

Show Supplier Material materials with Shrinkage, transverse of 0.5 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

EV/HEV Battery, Food Processor, Enclosures, Electronic Components, Circuit Protection, Data Management, Data Transfer, Document Handling, Meter Gas, Respiratory, Security/Detection, Small Appliance, Power Manangement, Wiring Devices, Wireless Communications

Availability

Americas

Processing methods

Maximum Moisture Content: 0.02%
Rear - Zone 1 Temperature: 225 to 275.0°C
Screw Speed: 20 to 100.0rpm
Mold Temperature: 70 to 95.0°C
Middle - Zone 2 Temperature: 240 to 280.0°C
Drying Temperature: 95 to 100.0°C
Shot to Cylinder Size: 30 to 70.0%
Vent Depth: 0.038 to 0.051mm
Melt Temperature: 260 to 290.0°C
Front - Zone 3 Temperature: 250 to 290.0°C
Drying Time: 3 to 4.0hrs
Nozzle Temperature: 260 to 290.0°C
Drying Time (Cumulative): 8hrs
Back Pressure: 0.3 to 0.7MPa

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.