General
Property | Temperature | Value | Comment |
---|---|---|---|
Relative density | 23.0 °C | 1.25 [-] Show Supplier Material materials with Relative density of 1.25 [-] | ASTM D 792 | |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 4 GPa Show Supplier Material materials with Elastic modulus of 4 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 3.7 % Show Supplier Material materials with Elongation of 3.7 % | ISO 527 | yield |
Flexural modulus | 23.0 °C | 3.8 GPa Show Supplier Material materials with Flexural modulus of 3.8 GPa | ISO 178 |
Flexural strength | 23.0 °C | 117 MPa Show Supplier Material materials with Flexural strength of 117 MPa | ISO 178 |
Impact strength, Charpy notched | 23.0 °C | 10 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 10 kJ/m² | ISO 179/2C | 23°C |
Impact strength, Izod notched | 23.0 °C | 9 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 9 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 131 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 131 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 2230 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 2230 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 443 J Show Supplier Material materials with Instrumented Impact, Total Energy of 443 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 57 MPa Show Supplier Material materials with Tensile strength of 57 MPa | ISO 527 | break |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 7.06E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 7.06E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 7.76E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 7.76E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 800 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 800 °C | IEC 60695-2-13 | 3.0 mm | |||
Heat deflection temperature | 111 - 126 °C Show Supplier Material materials with Heat deflection temperature of 111 - 126 °C | ||||
Heat deflection temperature, 0.45 MPa | 126 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 126 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 111 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 111 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Relative temperature index, electrical | 100 °C Show Supplier Material materials with Relative temperature index, electrical of 100 °C | UL 746B | |||
Relative temperature index, mechanical impact | 85 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 85 °C | UL 746B | |||
Relative temperature index, mechanical strength | 100 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 100 °C | UL 746B | |||
Vicat softening temperature | 132 °C Show Supplier Material materials with Vicat softening temperature of 132 °C | ISO 306 | Rate B/50 | |||
Flammability | UL Recognized, 94-5VA Flame Class Rating: ≥2mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> Radiant Panel Listing: TRUE- UL Tested <br> UV-light, water exposure/immersion: F1- UL 746C <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221170- - <br> Glow Wire Ignitability Temperature, 1.0 mm: 850°C IEC 60695-2-13 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 2 V Show Supplier Material materials with Comparative tracking index of 2 V | UL 746A | (UL) {PLC} |
Dielectric constant, 1MHz | 23.0 °C | 2.7 [-] Show Supplier Material materials with Dielectric constant, 1MHz of 2.7 [-] | ASTM D 150 |
Dielectric constant, 60Hz | 23.0 °C | 2.89 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.89 [-] | ASTM D 150 | 50/60 Hz |
Dielectric strength | 23.0 °C | 17.3 kV/mm Show Supplier Material materials with Dielectric strength of 17.3 kV/mm | ASTM D 149 | in oil, 3.2 mm |
Dissipation factor, 1MHz | 23.0 °C | 4.4E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 4.4E-3 [-] | ASTM D 150 |
Dissipation factor, 50Hz | 23.0 °C | 0.02 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 0.02 [-] | ASTM D 150 | 50/60 Hz |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 3 |
High Volt Arc Track Rate | 23.0 °C | 3 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 3 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
Sheet resistivity, ROA | 23.0 °C | 1.00E+16 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+16 Ω | >, ASTM D 257 |
Volume resistivity | 23.0 °C | 1.20E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 1.20E+16 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 7.6 g/10min Show Supplier Material materials with Melt mass-flow rate of 7.6 g/10min | ASTM D 1238 | 280°C/5.0 kgf | |
Melt volume-flow rate | 6 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 6 cm³/10min | ISO 1133 | MVR at 300°C/5.0 kg | |
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Medical Device, LED Lighting, Laundry Dryer, Meter Gas, Personal Computing, Non-LED Lighting, Oil/Gas, Security/Detection, Respiratory, Small Appliance, Power Manangement, Wireless Communications, Wiring Devices, Wearables, Washing Machine, Building Accessory, Battery Cell, Circuit Protection, Air Conditioning, Document Handling, Displays, Dishwasher, Data Transfer, Electronic Components, Enclosure/Housing/Cover, Enclosures, Individual Equiptment, Hygiene/Personal Care, Furnace/Heater, Food Processor | |
Availability | Americas | |
Processing methods | Shot to Cylinder Size: 30 to 70.0% | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |