General
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 5 % Show Supplier Material materials with Elongation of 5 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 7.8 GPa Show Supplier Material materials with Flexural modulus of 7.8 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Flexural strength | 23.0 °C | 172 MPa Show Supplier Material materials with Flexural strength of 172 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Tensile strength | 23.0 °C | 120 MPa Show Supplier Material materials with Tensile strength of 120 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.52E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.52E-5 1/K | ASTM E 831 | -40°C to 95°C | ||
Heat deflection temperature | 135 - 140 °C Show Supplier Material materials with Heat deflection temperature of 135 - 140 °C | ||||
Heat deflection temperature, 0.45 MPa | 140 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 140 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 135 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 135 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Relative temperature index, electrical | 110 °C Show Supplier Material materials with Relative temperature index, electrical of 110 °C | UL 746B | |||
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |||
Relative temperature index, mechanical strength | 110 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 110 °C | UL 746B | |||
Flammability | UL Recognized, 94V-1 Flame Class Rating: ≥0.71mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=228591- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=237105- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 3 V Show Supplier Material materials with Comparative tracking index of 3 V | UL 746A | (UL) {PLC} |
Dielectric constant, 60Hz | 23.0 °C | 3.15 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 3.15 [-] | ASTM D 150 | 50/60 Hz |
Dielectric strength | 23.0 °C | 20.8 kV/mm Show Supplier Material materials with Dielectric strength of 20.8 kV/mm | ASTM D 149 | in oil, 3.2 mm |
Dissipation factor, 50Hz | 23.0 °C | 2E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 2E-3 [-] | ASTM D 150 | 50/60 Hz |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 2 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.1 % Show Supplier Material materials with Shrinkage of 0.1 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Circuit Protection, Building Accessory, Cladding/Roof, Document Handling, Enclosures, Enclosure/Housing/Cover, Electronic Components, Hot Water System, Lawn/Garden, Fixture Bath/Shower, Furnace/Heater, Electronic Material Handling, Washing Machine, Wiring Devices, Wireless Communications, Motorcycle, Personal Care, Medical Device, LED Lighting, Surgical Devices, Small Appliance, Security/Detection, Renal and Blood Handling, Pump, Refrigerator | |
Availability | Europe,Asia,Americas | |
Processing methods | Mold Temperature: 80 to 110.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |