General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.11 g/cm³ Show Supplier Material materials with Density of 1.11 g/cm³ | ISO 1183 |
Limiting oxygen index | 23.0 °C | 30 % Show Supplier Material materials with Limiting oxygen index of 30 % | |
Moisture absorption | 23.0 °C | 0.05 % Show Supplier Material materials with Moisture absorption of 0.05 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.11 [-] Show Supplier Material materials with Relative density of 1.11 [-] | ASTM D 792 |
Water absorption | 23.0 °C | 0.18 % Show Supplier Material materials with Water absorption of 0.18 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2.5 GPa Show Supplier Material materials with Elastic modulus of 2.5 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 3.5 % Show Supplier Material materials with Elongation of 3.5 % | ISO 527 | yield, 50 mm/min |
Flexural modulus | 23.0 °C | 2.3 GPa Show Supplier Material materials with Flexural modulus of 2.3 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 87 MPa Show Supplier Material materials with Flexural strength of 87 MPa | ISO 178 | yield, 2 mm/min |
Impact strength, Charpy notched | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 5 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, 23°C |
Impact strength, Izod notched | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 6 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Tensile strength | 23.0 °C | 58 MPa Show Supplier Material materials with Tensile strength of 58 MPa | ISO 527 | yield, 50 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 8.3E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 8.3E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 7.7E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 7.7E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Glow Wire Ignition Temperature | 725 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 725 °C | IEC 60695-2-13 | 2.0 mm | |||
Heat deflection temperature | 85 °C Show Supplier Material materials with Heat deflection temperature of 85 °C | ||||
Heat deflection temperature, 1.80 MPa | 85 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 85 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | UL 746B | |||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | |||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | |||
Vicat softening temperature | 105 °C Show Supplier Material materials with Vicat softening temperature of 105 °C | ISO 306 | Rate B/50 | |||
Flammability | Glow Wire Flammability Index 960°C, passes at: 3mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3mm IEC 60695-2-12 <br> UL Recognized, 94V-1 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥2mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥1mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥1mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101271387- - <br> Glow Wire Ignitability Temperature, 1.0 mm: 700°C IEC 60695-2-13 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 250 V Show Supplier Material materials with Comparative tracking index of 250 V | IEC 60112 | |
Dielectric constant, 1MHz | 23.0 °C | 2.8 [-] Show Supplier Material materials with Dielectric constant, 1MHz of 2.8 [-] | IEC 60250 |
Dielectric strength | 23.0 °C | 27.5 kV/mm Show Supplier Material materials with Dielectric strength of 27.5 kV/mm | IEC 60243-1 | in oil, 1.6 mm |
Dissipation factor, 1MHz | 23.0 °C | 2E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 2E-3 [-] | IEC 60250 |
Sheet resistivity, ROA | 23.0 °C | 8.00E+16 - 8.50E+16 Ω Show Supplier Material materials with Sheet resistivity, ROA of 8.00E+16 - 8.50E+16 Ω | IEC 60093 |
Volume resistivity | 23.0 °C | 3.00E+16 - 3.50E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 3.00E+16 - 3.50E+16 Ω·cm | IEC 60093 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt volume-flow rate | 44 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 44 cm³/10min | ISO 1133 | MVR at 280°C/2.16 kg | |
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Displays | |
Availability | Americas | |
Processing methods | Drying Temperature: 70 to 80.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |