General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.08 g/cm³ Show Supplier Material materials with Density of 1.08 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 1.2 % Show Supplier Material materials with Moisture absorption of 1.2 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.08 [-] Show Supplier Material materials with Relative density of 1.08 [-] | ASTM D 792 |
Water absorption | 23.0 °C | 4.2 % Show Supplier Material materials with Water absorption of 4.2 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2 GPa Show Supplier Material materials with Elastic modulus of 2 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 4 % Show Supplier Material materials with Elongation of 4 % | ISO 527 | yield, 50 mm/min |
Flexural modulus | 23.0 °C | 1.9 GPa Show Supplier Material materials with Flexural modulus of 1.9 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 75 MPa Show Supplier Material materials with Flexural strength of 75 MPa | ISO 178 | yield, 2 mm/min |
Impact strength, Charpy notched | 23.0 °C | 18 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 18 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, 23°C |
Impact strength, Izod notched | 23.0 °C | 17 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 17 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 180 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 180 J/m | ASTM D 256 | notched, 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 50 J Show Supplier Material materials with Instrumented Impact, Total Energy of 50 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 50 MPa Show Supplier Material materials with Tensile strength of 50 MPa | ISO 527 | yield, 50 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 125°C +/- 2°C | |||
Coefficient of thermal expansion | 23.0 °C | 1E-4 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1E-4 1/K | ISO 11359-2 | 23°C to 60°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 9E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 9E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Heat deflection temperature | 175 °C Show Supplier Material materials with Heat deflection temperature of 175 °C | ||||
Heat deflection temperature, 0.45 MPa | 175 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 175 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Vicat softening temperature | 230 °C Show Supplier Material materials with Vicat softening temperature of 230 °C | ISO 306 | Rate A/50 | |||
Flammability | UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Volume resistivity | 23.0 °C | 1000 - 10000 Ω·cm Show Supplier Material materials with Volume resistivity of 1000 - 10000 Ω·cm | SABIC method |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 10 g/10min Show Supplier Material materials with Melt mass-flow rate of 10 g/10min | ASTM D 1238 | 280°C/5.0 kgf | |
Melt volume-flow rate | 12 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 12 cm³/10min | ISO 1133 | MVR at 280°C/5.0 kg | |
Shrinkage | 23.0 °C | 1.3 % Show Supplier Material materials with Shrinkage of 1.3 % | SABIC method | 3.2 mm |
Shrinkage, transverse | 23.0 °C | 1.1 % Show Supplier Material materials with Shrinkage, transverse of 1.1 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Auto Aftermarket, Dishwasher, Exterior Trim, Spoiler, Vertical Body Panel | |
Availability | Americas | |
Processing methods | Nozzle Temperature: 280 to 310.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |