General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.08 g/cm³ Show Supplier Material materials with Density of 1.08 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.64 % Show Supplier Material materials with Moisture absorption of 0.64 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.08 [-] Show Supplier Material materials with Relative density of 1.08 [-] | ASTM D 792 | |
Water absorption | 23.0 °C | 4.2 % Show Supplier Material materials with Water absorption of 4.2 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2.3 GPa Show Supplier Material materials with Elastic modulus of 2.3 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 40 % Show Supplier Material materials with Elongation of 40 % | ISO 527 | break, 50 mm/min |
Flexural modulus | 23.0 °C | 2.3 GPa Show Supplier Material materials with Flexural modulus of 2.3 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 90 MPa Show Supplier Material materials with Flexural strength of 90 MPa | ISO 178 | yield, 2 mm/min |
Impact strength, Charpy notched | 23.0 °C | 15 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 15 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, -30°C |
Impact strength, Izod notched | 23.0 °C | 22 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 22 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 180 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 180 J/m | ASTM D 256 | notched, -30°C |
Instrumented Impact, Total Energy | 23.0 °C | 60 J Show Supplier Material materials with Instrumented Impact, Total Energy of 60 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 60 MPa Show Supplier Material materials with Tensile strength of 60 MPa | ISO 527 | yield, 50 mm/min |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 9E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 9E-5 1/K | ISO 11359-2 | 23°C to 60°C |
Coefficient of thermal expansion, transverse | 23.0 °C | 9E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 9E-5 1/K | ISO 11359-2 | 23°C to 60°C |
Heat deflection temperature | 190 °C Show Supplier Material materials with Heat deflection temperature of 190 °C | ||
Heat deflection temperature, 0.45 MPa | 190 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 190 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |
Vicat softening temperature | 200 °C Show Supplier Material materials with Vicat softening temperature of 200 °C | ISO 306 | Rate B/120 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Volume resistivity | 23.0 °C | 1000 - 10000 Ω·cm Show Supplier Material materials with Volume resistivity of 1000 - 10000 Ω·cm | SABIC method |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 16 g/10min Show Supplier Material materials with Melt mass-flow rate of 16 g/10min | ASTM D 1238 | 280°C/5.0 kgf | |
Melt volume-flow rate | 19 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 19 cm³/10min | ISO 1133 | MVR at 280°C/5.0 kg | |
Shrinkage | 23.0 °C | 1.2 % Show Supplier Material materials with Shrinkage of 1.2 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Recreational Vehicle, Horizontal Body Panel, Vertical Body Panel, Heavy Vehicles, Exterior Trim, Exterior, Console, Auto Aftermarket | |
Availability | Europe,Asia,Americas | |
Processing methods | Maximum Moisture Content: 0.07% | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |