General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.46 g/cm³ Show Supplier Material materials with Density of 1.46 g/cm³ | ASTM D 792 |
Relative density | 23.0 °C | 1.46 [-] Show Supplier Material materials with Relative density of 1.46 [-] | ASTM D 792 | |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 14.8 GPa Show Supplier Material materials with Elastic modulus of 14.8 GPa | ASTM D 638 | 5 mm/min |
Elongation | 23.0 °C | 2.7 % Show Supplier Material materials with Elongation of 2.7 % | ASTM D 638 | yld, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 14.4 GPa Show Supplier Material materials with Flexural modulus of 14.4 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Flexural strength | 23.0 °C | 53 MPa Show Supplier Material materials with Flexural strength of 53 MPa | ASTM D 790 |
Impact strength, Izod notched | 23.0 °C | 87 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 87 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 87 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 87 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 826 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 826 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 153 MPa Show Supplier Material materials with Tensile strength of 153 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Thermal
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1.00E+5 - 1.00E+9 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+5 - 1.00E+9 Ω | ASTM D 257 |
Volume resistivity | 23.0 °C | 1.00E+5 - 1.00E+9 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+5 - 1.00E+9 Ω·cm | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Semiconductor | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120 to 150.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |