General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.08 g/cm³ Show Supplier Material materials with Density of 1.08 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.81 % Show Supplier Material materials with Moisture absorption of 0.81 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.09 [-] Show Supplier Material materials with Relative density of 1.09 [-] | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 1.6 GPa Show Supplier Material materials with Elastic modulus of 1.6 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 29 % Show Supplier Material materials with Elongation of 29 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 1.5 GPa Show Supplier Material materials with Flexural modulus of 1.5 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 49 MPa Show Supplier Material materials with Flexural strength of 49 MPa | ISO 178 |
Impact strength, Izod notched | 23.0 °C | 14 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 14 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 131 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 131 J/m | ASTM D 256 |
Instrumented Impact, Total Energy | 23.0 °C | 20 J Show Supplier Material materials with Instrumented Impact, Total Energy of 20 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 26 MPa Show Supplier Material materials with Tensile strength of 26 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1E-5 1/K | ASTM D 696 | -30°C to 30°C |
Coefficient of thermal expansion, transverse | 23.0 °C | 1.09E-4 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 1.09E-4 1/K | ASTM D 696 | -30°C to 30°C |
Heat deflection temperature | 66 - 77 °C Show Supplier Material materials with Heat deflection temperature of 66 - 77 °C | ||
Heat deflection temperature, 0.45 MPa | 77 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 77 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |
Heat deflection temperature, 1.80 MPa | 66 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 66 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1.00E+9 - 1.00E+11 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+9 - 1.00E+11 Ω | ASTM D 257 |
Volume resistivity | 23.0 °C | 1.00E+10 - 1.00E+12 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+10 - 1.00E+12 Ω·cm | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Non-LED Lighting, Pharmaceutical Manufacturing, Pharmaceutical Packaging & Drug Delivery | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 70 to 80.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |