General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.25 g/cm³ Show Supplier Material materials with Density of 1.25 g/cm³ | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elastic modulus | 23.0 °C | 2.8 GPa Show Supplier Material materials with Elastic modulus of 2.8 GPa | ASTM D 638 | 50 mm/min | ||
Elongation | 23.0 °C | 20 % Show Supplier Material materials with Elongation of 20 % | ASTM D 638 | break | ||
Flexural modulus | 23.0 °C | 2.8 GPa Show Supplier Material materials with Flexural modulus of 2.8 GPa | ASTM D 790 | ||
Flexural strength | 23.0 °C | 96 MPa Show Supplier Material materials with Flexural strength of 96 MPa | ASTM D 790 | ||
Impact strength, Izod notched | 23.0 °C | 106 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 106 kJ/m² | ASTM D 256 | notched, 23°C | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 106 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 106 J/m | ASTM D 256 | ||
Tensile strength | 23.0 °C | 58 MPa Show Supplier Material materials with Tensile strength of 58 MPa | ASTM D 638 | yield | ||
Impact strength, Izod unnotched, ASTM | ASTM D 4812 | 23°C |
Thermal
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1.00E+4 - 1.00E+7 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+4 - 1.00E+7 Ω | ASTM D 257 |
Volume resistivity | 23.0 °C | 1.00E+4 - 1.00E+7 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+4 - 1.00E+7 Ω·cm | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Application areas | Semiconductor | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |