NORYL™ NH6020 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS) designed for high heat resistance and thin-wall FR performance. This injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of 5VA at 2.5mm and V0 at 0.75mm along with UL746C Outdoor Suitability rating of F1 and RTI of 110C. NORYL NH6020 resin passes VDE/DIN 475 part 815 testing, Ball Pressure Test (BPT) at 125C, GWFI 960C at 1, 2, 3mm, GWIT 825C at 1mm, and CTI >600V making this an excellent candidate for unattended appliance components where EN/IEC 60335 applies.

This material data has been provided by Sabic.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.14 g/cm³

Show Supplier Material materials with Density of 1.14 g/cm³

ISO 1183

Moisture absorption

23.0 °C

0.06 %

Show Supplier Material materials with Moisture absorption of 0.06 %

ISO 62 | (23°C / 50% RH)

Relative density

23.0 °C

1.14 [-]

Show Supplier Material materials with Relative density of 1.14 [-]

ASTM D 792

Water absorption

23.0 °C

0.18 %

Show Supplier Material materials with Water absorption of 0.18 %

ISO 62-1 | (23°C/saturated)

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.7 GPa

Show Supplier Material materials with Elastic modulus of 2.7 GPa

ISO 527 | 1 mm/min

Elongation

23.0 °C

4.2 %

Show Supplier Material materials with Elongation of 4.2 %

ISO 527 | break, 50 mm/min

Flexural modulus

23.0 °C

2.7 GPa

Show Supplier Material materials with Flexural modulus of 2.7 GPa

ISO 178 | 2 mm/min

Flexural strength

23.0 °C

114 MPa

Show Supplier Material materials with Flexural strength of 114 MPa

ISO 178 | yield, 2 mm/min

Impact strength, Charpy notched

23.0 °C

9 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 9 kJ/m²

ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, 23°C

Impact strength, Izod notched

23.0 °C

8 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 8 kJ/m²

ISO 180/1A | notched 80*10*4, 23°C

Impact strength, Izod notched, ASTM

23.0 °C

49 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 49 J/m

ASTM D 256

Instrumented Impact, Total Energy

23.0 °C

18 J

Show Supplier Material materials with Instrumented Impact, Total Energy of 18 J

ASTM D 3763 | 23°C

Tensile strength

23.0 °C

56 MPa

Show Supplier Material materials with Tensile strength of 56 MPa

ISO 527 | break, 50 mm/min

Thermal

PropertyTemperatureValueComment

Ball Pressure Test

125.0

IEC 60695-10-2 | 125°C +/- 2°C

Coefficient of thermal expansion

23.0 °C

7.5E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 7.5E-5 1/K

ISO 11359-2 | -40°C to 40°C

Coefficient of thermal expansion, transverse

23.0 °C

7.75E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion, transverse of 7.75E-5 1/K

ISO 11359-2 | -40°C to 40°C

Glow Wire Flammability Index

960 °C

Show Supplier Material materials with Glow Wire Flammability Index of 960 °C

Glow Wire Ignition Temperature

800 °C

Show Supplier Material materials with Glow Wire Ignition Temperature of 800 °C

IEC 60695-2-13 | 3.0 mm

Heat deflection temperature

124 °C

Show Supplier Material materials with Heat deflection temperature of 124 °C

Heat deflection temperature, 1.80 MPa

124 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 124 °C

ISO 75/Af | Flatw 80*10*4 sp=64mm

Relative temperature index, electrical

110 °C

Show Supplier Material materials with Relative temperature index, electrical of 110 °C

UL 746B

Relative temperature index, mechanical impact

105 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C

UL 746B

Relative temperature index, mechanical strength

110 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 110 °C

UL 746B

Vicat softening temperature

151 °C

Show Supplier Material materials with Vicat softening temperature of 151 °C

ISO 306 | Rate B/120

Flammability

Glow Wire Ignitability Temperature, 1.0 mm: 825°C IEC 60695-2-13 <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: ≥2.5mm UL 94 <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 <br> UV-light, water exposure/immersion: F1- UL 746C <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100104907- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=100158888- -

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

600 V

Show Supplier Material materials with Comparative tracking index of 600 V

IEC 60112 |

Dielectric constant, 60Hz

23.0 °C

2.7 [-]

Show Supplier Material materials with Dielectric constant, 60Hz of 2.7 [-]

IEC 60250 | 50/60 Hz

Dielectric strength

23.0 °C

27 kV/mm

Show Supplier Material materials with Dielectric strength of 27 kV/mm

IEC 60243-1 | in oil, 1.6 mm

Dissipation factor, 1MHz

23.0 °C

2.9E-3 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 2.9E-3 [-]

IEC 60250

High Amp Arc Ignition

23.0 °C

1 mm

Show Supplier Material materials with High Amp Arc Ignition of 1 mm

≥, UL 746A | PLC 2

Hot-Wire Ignition

23.0 °C

1.5 mm

Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm

≥, UL 746A | PLC 1

Volume resistivity

23.0 °C

2.50E+16 - 4.20E+16 Ω·cm

Show Supplier Material materials with Volume resistivity of 2.50E+16 - 4.20E+16 Ω·cm

IEC 60093 |

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

13.5 g/10min

Show Supplier Material materials with Melt mass-flow rate of 13.5 g/10min

ASTM D 1238 | 280°C/5.0 kgf

Melt volume-flow rate

11 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 11 cm³/10min

ISO 1133 | MVR at 280°C/5.0 kg

Shrinkage

23.0 °C

0.5 %

Show Supplier Material materials with Shrinkage of 0.5 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Washing Machine, Pump, Freezer, Furnace/Heater, Electronic Components, Enclosures, Energy Management, Enclosure/Housing/Cover, Dishwasher, Displays, Cooking Range, Circuit Protection

Availability

Europe,Asia,Americas

Processing methods

Nozzle Temperature: 280 to 300.0°C
Rear - Zone 1 Temperature: 260 to 280.0°C
Middle - Zone 2 Temperature: 280 to 300.0°C
Drying Temperature: 110 to 120.0°C
Front - Zone 3 Temperature: 300 to 320.0°C
Drying Time: 2 to 3.0hrs
Melt Temperature: 300 to 320.0°C
Mold Temperature: 100 to 130.0°C
Hopper Temperature: 80 to 100.0°C

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.