General
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.42 - 0.52 [-] Show Supplier Material materials with Coefficient of friction of 0.42 - 0.52 [-] | ||
Coefficient of friction, kinetic | 0.42 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.42 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.52 [-] Show Supplier Material materials with Coefficient of friction, static of 0.52 [-] | ASTM D 3702 Modified: Manual | |
Density | 23.0 °C | 1.36 g/cm³ Show Supplier Material materials with Density of 1.36 g/cm³ | ISO 1183 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 4.5 GPa Show Supplier Material materials with Elastic modulus of 4.5 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 3.2 % Show Supplier Material materials with Elongation of 3.2 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 4.3 GPa Show Supplier Material materials with Flexural modulus of 4.3 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 109 MPa Show Supplier Material materials with Flexural strength of 109 MPa | ISO 178 | break, 2 mm/min |
Impact strength, Izod notched | 23.0 °C | 10 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 10 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod unnotched | 23.0 °C | 35 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 35 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Tensile strength | 23.0 °C | 75 MPa Show Supplier Material materials with Tensile strength of 75 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 4.6E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 4.6E-5 1/K | ISO 11359-2 | 23°C to 60°C |
Coefficient of thermal expansion, transverse | 23.0 °C | 7.4E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 7.4E-5 1/K | ISO 11359-2 | 23°C to 60°C |
Heat deflection temperature | 133 - 139 °C Show Supplier Material materials with Heat deflection temperature of 133 - 139 °C | ||
Heat deflection temperature, 0.45 MPa | 139 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 139 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |
Heat deflection temperature, 1.80 MPa | 133 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 133 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.2 % Show Supplier Material materials with Shrinkage of 0.2 % | SABIC method |
Technological properties
Property | ||
---|---|---|
Application areas | Lab Ware and Clinical Diagnostics | |
Availability | Europe,Americas | |
Processing methods | Melt Temperature: 305 to 325.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |