General
Property | Temperature | Value | Comment |
---|---|---|---|
Bulk density | 23.0 °C | 0.78 g/cm³ Show Supplier Material materials with Bulk density of 0.78 g/cm³ | ISO 1183 |
Limiting oxygen index | 23.0 °C | 47 % Show Supplier Material materials with Limiting oxygen index of 47 % | |
Water absorption | 23.0 °C | 1.25 % Show Supplier Material materials with Water absorption of 1.25 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 3.2 GPa Show Supplier Material materials with Elastic modulus of 3.2 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 60 % Show Supplier Material materials with Elongation of 60 % | ISO 527 | break, 50 mm/min |
Flexural modulus | 23.0 °C | 3.3 GPa Show Supplier Material materials with Flexural modulus of 3.3 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 160 MPa Show Supplier Material materials with Flexural strength of 160 MPa | ISO 178 | yield, 2 mm/min |
Hardness, Rockwell M | 23.0 °C | 109 [-] Show Supplier Material materials with Hardness, Rockwell M of 109 [-] | ASTM D 785 | |
Impact strength, Izod notched | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 6 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Taber Abrasion | 23.0 °C | 10 mg/1000cy Show Supplier Material materials with Taber Abrasion of 10 mg/1000cy | ASTM D 1044 | CS-17, 1 kg |
Tensile strength | 23.0 °C | 105 MPa Show Supplier Material materials with Tensile strength of 105 MPa | ISO 527 | yield, 50 mm/min |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 5E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 5E-5 1/K | ISO 11359-2 | 23°C to 150°C |
Coefficient of thermal expansion, transverse | 23.0 °C | 5E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 5E-5 1/K | ISO 11359-2 | 23°C to 150°C |
Heat deflection temperature | 190 - 200 °C Show Supplier Material materials with Heat deflection temperature of 190 - 200 °C | ||
Heat deflection temperature, 0.45 MPa | 200 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 200 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |
Heat deflection temperature, 1.80 MPa | 190 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 190 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |
Thermal conductivity | 23.0 °C | 0.24 W/(m·K) Show Supplier Material materials with Thermal conductivity of 0.24 W/(m·K) | ISO 8302 |
Vicat softening temperature | 211 °C Show Supplier Material materials with Vicat softening temperature of 211 °C | ISO 306 | Rate B/50 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric strength | 23.0 °C | 33 kV/mm Show Supplier Material materials with Dielectric strength of 33 kV/mm | IEC 60243-1 | in oil, 0.8 mm |
Dissipation factor | 23.0 °C | 2.5E-3 [-] Show Supplier Material materials with Dissipation factor of 2.5E-3 [-] | IEC 60250 | 2450 MHz |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | IEC 60093 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Composite | |
Availability | Europe,Americas | |
Processing methods | Drying Temperature: 150°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |