General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.25 g/cm³ Show Supplier Material materials with Density of 1.25 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.23 % Show Supplier Material materials with Moisture absorption of 0.23 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.25 [-] Show Supplier Material materials with Relative density of 1.25 [-] | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elastic modulus | 23.0 °C | 2.9 GPa Show Supplier Material materials with Elastic modulus of 2.9 GPa | ISO 527 | 1 mm/min | ||
Elongation | 23.0 °C | 20 % Show Supplier Material materials with Elongation of 20 % | ISO 527 | break, 5 mm/min | ||
Flexural modulus | 23.0 °C | 2.8 GPa Show Supplier Material materials with Flexural modulus of 2.8 GPa | ISO 178 | ||
Flexural strength | 23.0 °C | 100 MPa Show Supplier Material materials with Flexural strength of 100 MPa | ISO 178 | ||
Impact strength, Izod notched | 23.0 °C | 7.5 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 7.5 kJ/m² | ISO 180/1A | 80*10*4, 23°C | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 65.8 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 65.8 J/m | ASTM D 256 | ||
Instrumented Impact, Total Energy | 23.0 °C | 41 J Show Supplier Material materials with Instrumented Impact, Total Energy of 41 J | ASTM D 3763 | 23°C | ||
Tensile strength | 23.0 °C | 54 MPa Show Supplier Material materials with Tensile strength of 54 MPa | ISO 527 | break, 5 mm/min | ||
Impact strength, Izod unnotched | ISO 180/1U | unnotched 80*10*4 | ||||
Impact strength, Izod unnotched, ASTM | ASTM D 4812 | 23°C |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 6.2E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 6.2E-5 1/K | ASTM E 831 | -30°C to 30°C |
Coefficient of thermal expansion, transverse | 23.0 °C | 6.3E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 6.3E-5 1/K | ASTM E 831 | -30°C to 30°C |
Heat deflection temperature | 131 - 142 °C Show Supplier Material materials with Heat deflection temperature of 131 - 142 °C | ||
Heat deflection temperature, 0.45 MPa | 142 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 142 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |
Heat deflection temperature, 1.80 MPa | 131 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 131 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100 - 100000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100 - 100000 Ω | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Industrial Material Handling, Electronic Material Handling, Electronics, Semiconductor | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 121°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |