General
Property | Temperature | Value | Comment |
---|---|---|---|
Relative density | 23.0 °C | 1.32 [-] Show Supplier Material materials with Relative density of 1.32 [-] | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2.4 GPa Show Supplier Material materials with Elastic modulus of 2.4 GPa | ASTM D 638 | 5 mm/min |
Elongation | 23.0 °C | 20 % Show Supplier Material materials with Elongation of 20 % | SABIC - Japan Method | brk, Type I, 10 mm/min |
Flexural modulus | 23.0 °C | 2.3 GPa Show Supplier Material materials with Flexural modulus of 2.3 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Flexural strength | 23.0 °C | 77 MPa Show Supplier Material materials with Flexural strength of 77 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Impact strength, Izod notched | 23.0 °C | 41 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 41 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 41 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 41 J/m | ASTM D 256 | notched, 23°C |
Tensile strength | 23.0 °C | 46 MPa Show Supplier Material materials with Tensile strength of 46 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermal
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 9.00E+12 Ω Show Supplier Material materials with Sheet resistivity, ROA of 9.00E+12 Ω | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 30 g/10min Show Supplier Material materials with Melt mass-flow rate of 30 g/10min | ASTM D 1238 | 250°C/1.2 kgf | |
Shrinkage | 23.0 °C | 1.5 % Show Supplier Material materials with Shrinkage of 1.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Data Management | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 110°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |