General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 0.95 g/cm³ Show Supplier Material materials with Density of 0.95 g/cm³ | ISO 1183 |
Mechanical
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elastic modulus | 23.0 °C | 1.4 GPa Show Supplier Material materials with Elastic modulus of 1.4 GPa | ISO 527 | 1 mm/min | ||
Elongation | 23.0 °C | 8 % Show Supplier Material materials with Elongation of 8 % | ISO 527 | yield | ||
Flexural modulus | 23.0 °C | 1.4 GPa Show Supplier Material materials with Flexural modulus of 1.4 GPa | ISO 178 | ||
Flexural strength | 23.0 °C | 32 MPa Show Supplier Material materials with Flexural strength of 32 MPa | ISO 178 | ||
Impact strength, Izod notched | 23.0 °C | 10 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 10 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C | ||
Tensile strength | 23.0 °C | 28 MPa Show Supplier Material materials with Tensile strength of 28 MPa | ISO 527 | yield, 50 mm/min | ||
Impact strength, Izod unnotched | ISO 180/1U | 80*10*4, 23°C |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.1E-4 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.1E-4 1/K | ISO 11359-2 | -40°C to 40°C |
Coefficient of thermal expansion, transverse | 23.0 °C | 1.51E-4 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 1.51E-4 1/K | ISO 11359-2 | 23°C to 60°C |
Heat deflection temperature | 59 °C Show Supplier Material materials with Heat deflection temperature of 59 °C | ||
Heat deflection temperature, 1.80 MPa | 59 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 59 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1.00E+9 - 1.00E+11 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+9 - 1.00E+11 Ω | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Enclosures, Data Management, Conveyor | |
Availability | Europe,Americas | |
Processing methods | Drying Time: 4hrs | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |