General
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 1.38 - 1.6 [-] Show Supplier Material materials with Coefficient of friction of 1.38 - 1.6 [-] | ||
Coefficient of friction, kinetic | 1.6 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 1.6 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 1.38 [-] Show Supplier Material materials with Coefficient of friction, static of 1.38 [-] | ASTM D 3702 Modified: Manual | |
Density | 23.0 °C | 1.44 g/cm³ Show Supplier Material materials with Density of 1.44 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.03 % Show Supplier Material materials with Moisture absorption of 0.03 % | ISO 62 | (23°C / 50% RH) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 25.5 GPa Show Supplier Material materials with Elastic modulus of 25.5 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 1 % Show Supplier Material materials with Elongation of 1 % | ISO 527 | break |
Flexural modulus | 23.0 °C | 24.7 GPa Show Supplier Material materials with Flexural modulus of 24.7 GPa | ISO 178 |
Flexural strength | 23.0 °C | 311 MPa Show Supplier Material materials with Flexural strength of 311 MPa | ISO 178 |
Impact strength, Izod notched | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 5 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 49 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 49 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched | 23.0 °C | 28 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 28 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 437 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 437 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, at Peak | 23.0 °C | 3 J Show Supplier Material materials with Instrumented Impact, at Peak of 3 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 204 MPa Show Supplier Material materials with Tensile strength of 204 MPa | ISO 527 | break |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 8.7E-6 1/K Show Supplier Material materials with Coefficient of thermal expansion of 8.7E-6 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 4.08E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 4.08E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |||
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | UL 746B | |||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | |||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101284689- - <br> UL Recognized, 94V-0 Flame Class Rating: 1mm UL 94 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100 - 1000000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100 - 1000000 Ω | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Weapon | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120 to 150.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |