General
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 3.6 GPa Show Supplier Material materials with Elastic modulus of 3.6 GPa | ASTM D 638 | 5 mm/min |
Elongation | 23.0 °C | 60 % Show Supplier Material materials with Elongation of 60 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 3.5 GPa Show Supplier Material materials with Flexural modulus of 3.5 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Flexural strength | 23.0 °C | 165 MPa Show Supplier Material materials with Flexural strength of 165 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Impact strength, Izod notched | 23.0 °C | 32 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 32 kJ/m² | ASTM D 256 | notched, 23°C |
Taber Abrasion | 23.0 °C | 10 mg/1000cy Show Supplier Material materials with Taber Abrasion of 10 mg/1000cy | ASTM D 1044 | CS-17, 1 kg |
Tensile strength | 23.0 °C | 110 MPa Show Supplier Material materials with Tensile strength of 110 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 5.58E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 5.58E-5 1/K | ASTM E 831 | -20°C to 150°C | ||
Heat deflection temperature | 198 - 207 °C Show Supplier Material materials with Heat deflection temperature of 198 - 207 °C | ||||
Heat deflection temperature, 0.45 MPa | 207 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 207 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 198 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 198 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Relative temperature index, electrical | 170 °C Show Supplier Material materials with Relative temperature index, electrical of 170 °C | UL 746B | |||
Relative temperature index, mechanical impact | 170 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 170 °C | UL 746B | |||
Relative temperature index, mechanical strength | 170 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 170 °C | UL 746B | |||
Thermal conductivity | 23.0 °C | 0.22 W/(m·K) Show Supplier Material materials with Thermal conductivity of 0.22 W/(m·K) | ASTM C177 | ||
Vicat softening temperature | 218 °C Show Supplier Material materials with Vicat softening temperature of 218 °C | ASTM D 1525 | Rate B/50 | |||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101048269- - <br> UL Recognized, 94-5VA Flame Class Rating: ≥3mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> NBS Smoke Density, Flaming, Ds 4 min: 2- ASTM E 662 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 4 V Show Supplier Material materials with Comparative tracking index of 4 V | UL 746A | (UL) {PLC} |
Dielectric strength | 23.0 °C | 28 kV/mm Show Supplier Material materials with Dielectric strength of 28 kV/mm | ASTM D 149 | in oil, 1.6 mm |
Dissipation factor | 23.0 °C | 2.5E-3 [-] Show Supplier Material materials with Dissipation factor of 2.5E-3 [-] | ASTM D 150 | 2450 MHz |
High Amp Arc Ignition | 23.0 °C | 0.75 mm Show Supplier Material materials with High Amp Arc Ignition of 0.75 mm | ≥, UL 746A | PLC 4 |
High Volt Arc Track Rate | 23.0 °C | 2 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 1 |
Volume resistivity | 23.0 °C | 1.00E+17 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+17 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Tray, Surgical Tray, Sunglasses, Wiring Devices, Wearables, Water Treatment/Filtration, Wireless Communications, Pipe/Fitting, Rear/Signal Lighting, Photo/Video Camera, Pharmaceutical Packaging & Drug Delivery, Power Manangement, Photovoltaic Components, Respiratory, Safety Glasses, Semiconductor, Security/Detection, Surgical Devices, Small Appliance, Smart/ID Card, Ignition System, Interior Rail Components, Meter Gas, Monitoring and Imaging, Medical Device, LED Lighting, Personal Computing, Oil/Gas, Personal Care, OLED, Lighting, Non-LED Lighting, Enclosure/Housing/Cover, Electronics, Enclosures, Electronic Components, Lab Ware and Clinical Diagnostics, Individual Equiptment, Industrial Material Handling, Fuel Cell, Gas/Electric Oven, Humidity Control, Eyeglasses, Front Grille, Forward Lighting, Food Processor, Food Container, Fog Lamp, Fluid Delivery, Exterior Rail Components, Electronic Material Handling, Engine Cooling System, Exterior Trim, Air Cabin Interiors, Aircraft Seating, Aerospace, Auto Electrical, Building Accessory, Circuit Protection, Audio, Auto Aftermarket, Composite, Commercial Storage/Cookware, Cooking Range, Coffee Maker/Espresso Machine, Data Transfer, Data Management, Displays, Dishwasher, Document Handling, Wire & cable, Adhesives | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 150°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |