General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.61 g/cm³ Show Supplier Material materials with Density of 1.61 g/cm³ | ISO 1183 |
Limiting oxygen index | 23.0 °C | 48 % Show Supplier Material materials with Limiting oxygen index of 48 % | |
Moisture absorption | 23.0 °C | 0.4 % Show Supplier Material materials with Moisture absorption of 0.4 % | ISO 62 | (23°C / 50% RH) |
Water absorption | 23.0 °C | 0.8 % Show Supplier Material materials with Water absorption of 0.8 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 11.5 GPa Show Supplier Material materials with Elastic modulus of 11.5 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 2 % Show Supplier Material materials with Elongation of 2 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 10 GPa Show Supplier Material materials with Flexural modulus of 10 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 240 MPa Show Supplier Material materials with Flexural strength of 240 MPa | ISO 178 | break, 2 mm/min |
Hardness, Ball Indentation | 23.0 °C | 170 MPa Show Supplier Material materials with Hardness, Ball Indentation of 170 MPa | ISO 2039-1 | H358/30 |
Impact strength, Charpy unnotched | 23.0 °C | 40 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 40 kJ/m² | ISO 179/1eU | Unnotch Edgew 80*10*4 sp=62mm, -30°C |
Impact strength, Izod unnotched | 23.0 °C | 35 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 35 kJ/m² | ISO 180/1U | unnotched 80*10*4, -30°C |
Taber Abrasion | 23.0 °C | 20 mg/1000cy Show Supplier Material materials with Taber Abrasion of 20 mg/1000cy | SABIC method | CS-17, 1 kg |
Tensile strength | 23.0 °C | 180 MPa Show Supplier Material materials with Tensile strength of 180 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 125°C +/- 2°C | |||
Coefficient of thermal expansion | 23.0 °C | 1.5E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.5E-5 1/K | ISO 11359-2 | 23°C to 150°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 4.5E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 4.5E-5 1/K | ISO 11359-2 | 23°C to 150°C | ||
Heat deflection temperature | 210 - 215 °C Show Supplier Material materials with Heat deflection temperature of 210 - 215 °C | ||||
Heat deflection temperature, 0.45 MPa | 215 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 215 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 210 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 210 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Relative temperature index, electrical | 170 °C Show Supplier Material materials with Relative temperature index, electrical of 170 °C | UL 746B | |||
Relative temperature index, mechanical impact | 170 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 170 °C | UL 746B | |||
Relative temperature index, mechanical strength | 170 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 170 °C | UL 746B | |||
Thermal conductivity | 23.0 °C | 0.33 W/(m·K) Show Supplier Material materials with Thermal conductivity of 0.33 W/(m·K) | ISO 8302 | ||
Vicat softening temperature | 230 °C Show Supplier Material materials with Vicat softening temperature of 230 °C | ISO 306 | Rate A/50 | |||
Flammability | UL Recognized, 94V-0 Flame Class Rating: ≥0.25mm UL 94 <br> Glow Wire Ignitability Temperature, 1.5 mm: 875°C IEC 60695-2-13 <br> Glow Wire Ignitability Temperature, 1.0 mm: 850°C IEC 60695-2-13 <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221103- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 5 V Show Supplier Material materials with Comparative tracking index of 5 V | UL 746A | (UL) {PLC} |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 4 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt volume-flow rate | 5 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 5 cm³/10min | ISO 1133 | MVR at 360°C/5.0 kg | |
Shrinkage | 23.0 °C | 0.1 % Show Supplier Material materials with Shrinkage of 0.1 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Meter Gas | |
Availability | Europe | |
Processing methods | Drying Time: 4 to 6.0hrs | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |