LNP™ COLORCOMP™ Compound W1000EXP - Americas

Want to keep this datasheet? Save it now in your required format

Description

LNP* COLORCOMP* W1000EXP is an unreinforced compound based on PBT resin. Added feature of this grade is a typical viscosity of 5000-7000.

This material data has been provided by Sabic.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Relative density

23.0 °C

1.31 [-]

Show Supplier Material materials with Relative density of 1.31 [-]

ASTM D 792

Specific volume

23.0 °C

0.76 cm³/g

Show Supplier Material materials with Specific volume of 0.76 cm³/g

ASTM D 792

Water absorption

23.0 °C

0.08 %

Show Supplier Material materials with Water absorption of 0.08 %

ASTM D 570 | (23°C/24hrs)

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

200 %

Show Supplier Material materials with Elongation of 200 %

ASTM D 638 | brk, Type I, 50 mm/min

Flexural modulus

23.0 °C

2.3 GPa

Show Supplier Material materials with Flexural modulus of 2.3 GPa

ASTM D 790 | 1.3 mm/min, 50 mm span

Flexural strength

23.0 °C

82 MPa

Show Supplier Material materials with Flexural strength of 82 MPa

ASTM D 790 | yld, 1.3 mm/min, 50 mm span

Gardner Impact

23.0 °C

40 J

Show Supplier Material materials with Gardner Impact of 40 J

ASTM D 3029 | modified, 23°C

Hardness, Rockwell R

23.0 °C

117 [-]

Show Supplier Material materials with Hardness, Rockwell R of 117 [-]

ASTM D 785

Impact strength, Izod notched

23.0 °C

53 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 53 kJ/m²

ASTM D 256 | notched, 23°C

Impact strength, Izod notched, ASTM

23.0 °C

53 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 53 J/m

ASTM D 256 | notched, 23°C

Impact strength, Izod unnotched, ASTM

23.0 °C

1602 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1602 J/m

ASTM D 4812 | 23°C

Tensile strength

23.0 °C

51 MPa

Show Supplier Material materials with Tensile strength of 51 MPa

ASTM D 638 | brk, Type I, 50 mm/min

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.39E-4 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.39E-4 1/K

ASTM E 831 | 60°C to 138°C

Heat deflection temperature

54 - 154 °C

Show Supplier Material materials with Heat deflection temperature of 54 - 154 °C

Heat deflection temperature, 0.45 MPa

154 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 154 °C

ASTM D 648 | 6.4 mm, unannealed

Heat deflection temperature, 1.80 MPa

54 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 54 °C

ASTM D 648 | 6.4 mm, unannealed

Relative temperature index, electrical

120 °C

Show Supplier Material materials with Relative temperature index, electrical of 120 °C

UL 746B

Relative temperature index, mechanical impact

120 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 120 °C

UL 746B

Relative temperature index, mechanical strength

140 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C

UL 746B

Flammability

UL Recognized, 94HB Flame Class Rating: ≥0.84mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=103952988- -

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

0 V

Show Supplier Material materials with Comparative tracking index of 0 V

UL 746A | (UL) {PLC}

Dielectric constant, 100Hz

23.0 °C

3.3 [-]

Show Supplier Material materials with Dielectric constant, 100Hz of 3.3 [-]

ASTM D 150

Dielectric constant, 1MHz

23.0 °C

3.1 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 3.1 [-]

ASTM D 150

Dielectric strength

23.0 °C

15.7 kV/mm

Show Supplier Material materials with Dielectric strength of 15.7 kV/mm

ASTM D 149 | in oil, 3.2 mm

Dissipation factor, 100Hz

23.0 °C

2E-3 [-]

Show Supplier Material materials with Dissipation factor, 100Hz of 2E-3 [-]

ASTM D 150

Dissipation factor, 1MHz

23.0 °C

0.02 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 0.02 [-]

ASTM D 150

High Amp Arc Ignition

23.0 °C

1.5 mm

Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm

≥, UL 746A | PLC 0

High Volt Arc Track Rate

23.0 °C

1 PLC Code

Show Supplier Material materials with High Volt Arc Track Rate of 1 PLC Code

UL 746A | (PLC)

Hot-Wire Ignition

23.0 °C

1.5 mm

Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm

≥, UL 746A | PLC 4

Volume resistivity

23.0 °C

4.00E+16 Ω·cm

Show Supplier Material materials with Volume resistivity of 4.00E+16 Ω·cm

>, ASTM D 257

Rheological Properties

PropertyTemperatureValueComment

Melt viscosity

23.0 °C

600 Pa·s

Show Supplier Material materials with Melt viscosity of 600 Pa·s

SABIC method

Shrinkage

23.0 °C

1.5 %

Show Supplier Material materials with Shrinkage of 1.5 %

SABIC method | 2.3-4.6 mm

Shrinkage, transverse

23.0 °C

1 %

Show Supplier Material materials with Shrinkage, transverse of 1 %

SABIC method | 0.75-2.3 mm

Technological properties

Property
Availability

Americas

Processing methods

Drying Temperature: 120°C
Drying Time: 3 to 4.0hrs
Drying Time (Cumulative): 12hrs
Maximum Moisture Content: 0.02%
Melt Temperature: 245 to 260.0°C
Nozzle Temperature: 240 to 255.0°C
Front - Zone 3 Temperature: 245 to 260.0°C
Middle - Zone 2 Temperature: 240 to 255.0°C
Rear - Zone 1 Temperature: 230 to 250.0°C
Mold Temperature: 50 to 75.0°C
Back Pressure: 0.3 to 0.7MPa
Screw Speed: 50 to 100.0rpm
Shot to Cylinder Size: 40 to 80.0%
Vent Depth: 0.013 to 0.025mm

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.