Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.57 - 0.66 [-] Show Supplier Material materials with Coefficient of friction of 0.57 - 0.66 [-] | ||
Coefficient of friction, kinetic | 0.66 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.66 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.57 [-] Show Supplier Material materials with Coefficient of friction, static of 0.57 [-] | ASTM D 3702 Modified: Manual | |
Density | 23.0 °C | 1.43 g/cm³ Show Supplier Material materials with Density of 1.43 g/cm³ | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 3.3 % Show Supplier Material materials with Elongation of 3.3 % | ASTM D 638 | break |
Flexural modulus | 23.0 °C | 9.3 GPa Show Supplier Material materials with Flexural modulus of 9.3 GPa | ASTM D 790 |
Flexural strength | 23.0 °C | 275 MPa Show Supplier Material materials with Flexural strength of 275 MPa | ASTM D 790 |
Impact strength, Izod notched | 23.0 °C | 128 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 128 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 128 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 128 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1121 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1121 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 185 MPa Show Supplier Material materials with Tensile strength of 185 MPa | ASTM D 638 | break |
Thermal
Technological properties
Property | ||
---|---|---|
Application areas | Document Handling, Electronics | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |