General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.11 g/cm³ Show Supplier Material materials with Density of 1.11 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.28 % Show Supplier Material materials with Moisture absorption of 0.28 % | ASTM D 570 | (23°C/50% RH/24 hrs) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 52.7 % Show Supplier Material materials with Elongation of 52.7 % | ASTM D 638 | break |
Flexural modulus | 23.0 °C | 1.7 GPa Show Supplier Material materials with Flexural modulus of 1.7 GPa | ASTM D 790 |
Flexural strength | 23.0 °C | 54 MPa Show Supplier Material materials with Flexural strength of 54 MPa | ASTM D 790 |
Impact strength, Izod notched | 23.0 °C | 603 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 603 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 603 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 603 J/m | ASTM D 256 |
Tensile strength | 23.0 °C | 31 MPa Show Supplier Material materials with Tensile strength of 31 MPa | ASTM D 638 | break |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.17E-4 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.17E-4 1/K | ASTM E 831 | -40°C to 40°C |
Coefficient of thermal expansion, transverse | 23.0 °C | 1.17E-4 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 1.17E-4 1/K | ASTM E 831 | -40°C to 40°C |
Heat deflection temperature | 55 °C Show Supplier Material materials with Heat deflection temperature of 55 °C | ||
Heat deflection temperature, 1.80 MPa | 55 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 55 °C | ASTM D 648 | 3.2mm, unannealed |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100 - 10000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100 - 10000 Ω | ASTM D 257 |
Volume resistivity | 23.0 °C | 100 - 10000 Ω·cm Show Supplier Material materials with Volume resistivity of 100 - 10000 Ω·cm | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Application areas | Oil/Gas | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |