General
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2.2 GPa Show Supplier Material materials with Elastic modulus of 2.2 GPa | ASTM D 638 | 5 mm/min |
Elongation | 23.0 °C | 6 % Show Supplier Material materials with Elongation of 6 % | ASTM D 638 | yld, Type I, 50 mm/min |
Flexural modulus | 23.0 °C | 2.1 GPa Show Supplier Material materials with Flexural modulus of 2.1 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Flexural strength | 23.0 °C | 90 MPa Show Supplier Material materials with Flexural strength of 90 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Impact strength, Izod notched | 23.0 °C | 800 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 800 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 650 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 650 J/m | ASTM D 256 | -40°C |
Instrumented Impact, Total Energy | 23.0 °C | 70 J Show Supplier Material materials with Instrumented Impact, Total Energy of 70 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 57 MPa Show Supplier Material materials with Tensile strength of 57 MPa | ASTM D 638 | yld, Type I, 50 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 6E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 6E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 6E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 6E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Glow Wire Flammability Index | 825 °C Show Supplier Material materials with Glow Wire Flammability Index of 825 °C | ||||
Glow Wire Ignition Temperature | 850 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 850 °C | IEC 60695-2-13 | 0.75 mm | |||
Heat deflection temperature | 123 °C Show Supplier Material materials with Heat deflection temperature of 123 °C | ||||
Heat deflection temperature, 1.80 MPa | 123 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 123 °C | ASTM D 648 | 3.2mm, unannealed | |||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Vicat softening temperature | 145 °C Show Supplier Material materials with Vicat softening temperature of 145 °C | ASTM D 1525 | Rate B/50 | |||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100656422- - <br> UL Recognized, 94HB Flame Class Rating: ≥0.75mm UL 94 <br> Glow Wire Ignitability Temperature, 1.5 mm: 875°C IEC 60695-2-13 <br> Glow Wire Ignitability Temperature, 1.0 mm: 875°C IEC 60695-2-13 <br> Glow Wire Flammability Index, 1.5 mm: 850°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 1.0 mm: 850°C IEC 60695-2-12 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 1MHz | 23.0 °C | 3 [-] Show Supplier Material materials with Dielectric constant, 1MHz of 3 [-] | ASTM D 150 |
Dielectric strength | 23.0 °C | 15 kV/mm Show Supplier Material materials with Dielectric strength of 15 kV/mm | ASTM D 149 | in oil, 0.8 mm |
Dissipation factor, 1MHz | 23.0 °C | 9.2E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 9.2E-3 [-] | ASTM D 150 | |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 3 |
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | >, ASTM D 257 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | >, ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 15 g/10min Show Supplier Material materials with Melt mass-flow rate of 15 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Shrinkage | 23.0 °C | 0.4 % Show Supplier Material materials with Shrinkage of 0.4 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Enclosures | |
Availability | Europe,Asia | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |