General
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 3 GPa Show Supplier Material materials with Elastic modulus of 3 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 3.2 % Show Supplier Material materials with Elongation of 3.2 % | ISO 527 | yield, 50 mm/min |
Flexural modulus | 23.0 °C | 2.6 GPa Show Supplier Material materials with Flexural modulus of 2.6 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 107 MPa Show Supplier Material materials with Flexural strength of 107 MPa | ISO 178 | yield, 2 mm/min |
Impact strength, Izod notched | 23.0 °C | 10 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 10 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 213 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 213 J/m | ASTM D 256 | notched, 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 31 J Show Supplier Material materials with Instrumented Impact, Total Energy of 31 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 61 MPa Show Supplier Material materials with Tensile strength of 61 MPa | ISO 527 | break, 50 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 7.74E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 7.74E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 8.1E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 8.1E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Heat deflection temperature | 82 - 95 °C Show Supplier Material materials with Heat deflection temperature of 82 - 95 °C | ||||
Heat deflection temperature, 0.45 MPa | 95 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 95 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 82 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 82 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 50 °C Show Supplier Material materials with Relative temperature index, electrical of 50 °C | UL 746B | |||
Relative temperature index, mechanical impact | 50 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C | UL 746B | |||
Relative temperature index, mechanical strength | 50 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C | UL 746B | |||
Vicat softening temperature | 108 °C Show Supplier Material materials with Vicat softening temperature of 108 °C | ISO 306 | Rate B/120 | |||
Flammability | UL Recognized, 94V-0 Flame Class Rating: 1.5mm UL 94 <br> UL Recognized, 94HB Flame Class Rating: 0.99mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: 3mm UL 94 <br> UV-light, water exposure/immersion: F2- UL 746C |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 2 V Show Supplier Material materials with Comparative tracking index of 2 V | UL 746A | (UL) {PLC} |
High Amp Arc Ignition | 23.0 °C | 2 mm Show Supplier Material materials with High Amp Arc Ignition of 2 mm | UL 746A | surface {PLC} |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 2 mm Show Supplier Material materials with Hot-Wire Ignition of 2 mm | UL 746A | (PLC) |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 18 g/10min Show Supplier Material materials with Melt mass-flow rate of 18 g/10min | ASTM D 1238 | 260°C/3.8 kgf | |
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Document Handling | |
Availability | Europe,Asia,Americas | |
Processing methods | Melt Temperature: 250 to 275.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |