Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2.6 GPa Show Supplier Material materials with Elastic modulus of 2.6 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 4.5 % Show Supplier Material materials with Elongation of 4.5 % | ISO 527 | yield, 50 mm/min |
Flexural modulus | 23.0 °C | 2.5 GPa Show Supplier Material materials with Flexural modulus of 2.5 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 109 MPa Show Supplier Material materials with Flexural strength of 109 MPa | ISO 178 | yield, 2 mm/min |
Impact strength, Izod notched | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 6 kJ/m² | ISO 180/1A | notched 80*10*4, -30°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 100 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 100 J/m | ASTM D 256 | notched, 23°C |
Tensile strength | 23.0 °C | 55 MPa Show Supplier Material materials with Tensile strength of 55 MPa | ISO 527 | break, 50 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 7E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 7E-5 1/K | TMA | -30°C to 30°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 6.8E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 6.8E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Heat deflection temperature | 119 - 135 °C Show Supplier Material materials with Heat deflection temperature of 119 - 135 °C | ||||
Heat deflection temperature, 0.45 MPa | 135 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 135 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 119 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 119 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 110 °C Show Supplier Material materials with Relative temperature index, electrical of 110 °C | UL 746B | |||
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |||
Relative temperature index, mechanical strength | 110 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 110 °C | UL 746B | |||
Vicat softening temperature | 139 °C Show Supplier Material materials with Vicat softening temperature of 139 °C | ISO 306 | Rate B/120 | |||
Flammability | UL Recognized, 94-5VA Flame Class Rating: ≥2.5mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100037004- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 2 V Show Supplier Material materials with Comparative tracking index of 2 V | UL 746A | (UL) {PLC} |
High Amp Arc Ignition | 23.0 °C | 0.75 mm Show Supplier Material materials with High Amp Arc Ignition of 0.75 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 0.75 mm Show Supplier Material materials with Hot-Wire Ignition of 0.75 mm | ≥, UL 746A | PLC 0 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Enclosures, Energy Management, Enclosure/Housing/Cover, EV/HEV Battery, Battery Pack, Battery Cell, Audio, Air Conditioning, Document Handling, Displays, Dishwasher, Data Transfer, Power Manangement, Photovoltaic Components, Medical Device, LED Lighting, Personal Computing, Wiring Devices | |
Availability | Europe,Asia,Americas | |
Processing methods | Vent Depth: 0.038 to 0.051mm | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |