General
Property | Temperature | Value | Comment |
---|---|---|---|
Water absorption | 23.0 °C | 2.02 % Show Supplier Material materials with Water absorption of 2.02 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 46 % Show Supplier Material materials with Elongation of 46 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 1.9 GPa Show Supplier Material materials with Flexural modulus of 1.9 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 89 MPa Show Supplier Material materials with Flexural strength of 89 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Impact strength, Izod notched | 23.0 °C | 18 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 18 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Taber Abrasion | 23.0 °C | 19 mg/1000cy Show Supplier Material materials with Taber Abrasion of 19 mg/1000cy | ASTM D 1044 | CS-17, 1 kg |
Tensile strength | 23.0 °C | 54 MPa Show Supplier Material materials with Tensile strength of 54 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 9E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 9E-5 1/K | ASTM E 831 | -20°C to 150°C |
Heat deflection temperature | 150 °C Show Supplier Material materials with Heat deflection temperature of 150 °C | ||
Heat deflection temperature, 0.45 MPa | 150 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 150 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |
Vicat softening temperature | 170 °C Show Supplier Material materials with Vicat softening temperature of 170 °C | ISO 306 | Rate B/120 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.9 % Show Supplier Material materials with Shrinkage of 0.9 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Wheel Cover, Recreational Vehicle, Auto Aftermarket | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 95 to 105.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |