Property | Temperature | Value | Comment |
---|---|---|---|
Water absorption | 23.0 °C | 3.5 % Show Supplier Material materials with Water absorption of 3.5 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 8 % Show Supplier Material materials with Elongation of 8 % | ISO 527 | yield, 50 mm/min |
Flexural modulus | 23.0 °C | 2.2 GPa Show Supplier Material materials with Flexural modulus of 2.2 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 70 MPa Show Supplier Material materials with Flexural strength of 70 MPa | ISO 178 | yield, 2 mm/min |
Impact strength, Izod notched | 23.0 °C | 13 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 13 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Taber Abrasion | 23.0 °C | 15 mg/1000cy Show Supplier Material materials with Taber Abrasion of 15 mg/1000cy | SABIC method | CS-17, 1 kg |
Tensile strength | 23.0 °C | 55 MPa Show Supplier Material materials with Tensile strength of 55 MPa | ISO 527 | yield, 50 mm/min |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 9E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 9E-5 1/K | ISO 11359-2 | 23°C to 60°C |
Heat deflection temperature | 154 °C Show Supplier Material materials with Heat deflection temperature of 154 °C | ||
Heat deflection temperature, 0.45 MPa | 154 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 154 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |
Vicat softening temperature | 166 °C Show Supplier Material materials with Vicat softening temperature of 166 °C | ISO 306 | Rate B/50 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.9 % Show Supplier Material materials with Shrinkage of 0.9 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Wheel Cover, Recreational Vehicle, Auto Aftermarket | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 100 to 120.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |