General
Property | Temperature | Value | Comment |
---|---|---|---|
Limiting oxygen index | 23.0 °C | 27 % Show Supplier Material materials with Limiting oxygen index of 27 % | |
Relative density | 23.0 °C | 1.23 [-] Show Supplier Material materials with Relative density of 1.23 [-] | ASTM D 792 | |
Water absorption | 23.0 °C | 0.06 % Show Supplier Material materials with Water absorption of 0.06 % | ASTM D 570 | (23°C/24hrs) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 5 % Show Supplier Material materials with Elongation of 5 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 5.7 GPa Show Supplier Material materials with Flexural modulus of 5.7 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Flexural strength | 23.0 °C | 151 MPa Show Supplier Material materials with Flexural strength of 151 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Tensile strength | 23.0 °C | 106 MPa Show Supplier Material materials with Tensile strength of 106 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 3.6E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 3.6E-5 1/K | ASTM E 831 | -40°C to 95°C | ||
Heat deflection temperature | 132 - 137 °C Show Supplier Material materials with Heat deflection temperature of 132 - 137 °C | ||||
Heat deflection temperature, 0.45 MPa | 137 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 137 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 132 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 132 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Relative temperature index, electrical | 110 °C Show Supplier Material materials with Relative temperature index, electrical of 110 °C | UL 746B | |||
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |||
Relative temperature index, mechanical strength | 110 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 110 °C | UL 746B | |||
Flammability | UL Recognized, 94V-0 Flame Class Rating: 5.99mm UL 94 <br> UL Recognized, 94V-1 Flame Class Rating: 1.47mm UL 94 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 1 V Show Supplier Material materials with Comparative tracking index of 1 V | UL 746A | (UL) {PLC} |
Dielectric constant, 60Hz | 23.0 °C | 2.98 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.98 [-] | ASTM D 150 | 50/60 Hz |
Dielectric strength | 23.0 °C | 23.6 kV/mm Show Supplier Material materials with Dielectric strength of 23.6 kV/mm | ASTM D 149 | in oil, 3.2 mm |
Dissipation factor, 50Hz | 23.0 °C | 1.6E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 1.6E-3 [-] | ASTM D 150 | 50/60 Hz |
High Amp Arc Ignition | 23.0 °C | 1 mm Show Supplier Material materials with High Amp Arc Ignition of 1 mm | UL 746A | surface {PLC} |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 0 mm Show Supplier Material materials with Hot-Wire Ignition of 0 mm | UL 746A | (PLC) |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.2 % Show Supplier Material materials with Shrinkage of 0.2 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Enclosure/Housing/Cover, Energy Management, Electronics, Enclosures, Electronic Components, EV Infrastructure, Electronic Material Handling, EV/HEV Battery, Fixture Bath/Shower, Industrial Material Handling, Individual Equiptment, Hygiene/Personal Care, HVAC Underhood, Lab Ware and Clinical Diagnostics, Hot Water System, Humidity Control, Heavy Vehicles, Cluster, Coffee Maker/Espresso Machine, Battery System, Building Element, Data Transfer, Document Handling, Displays, Dishwasher, Defense Vehicles, Drain Pan, Air Conditioning, Battery Pack, Building Accessory, Circuit Protection, Audio, Auto Aftermarket, ATM/Ticket Machine, Security/Detection, Respiratory, Sensor, Surgical Devices, Pump, Pipe/Fitting, Power Manangement, Plumbing, Photovoltaic Components, Ignition System, Meter Gas, Microwave Oven, Personal Computing, Non-LED Lighting, Motorcycle, Wearables, Water Treatment/Filtration, Wiring Devices, Wireless Communications, Washing Machine, Travel Suitcase, Swimming Pool/Spa, Traffic Management | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 110 to 120.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |