General
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 40 % Show Supplier Material materials with Elongation of 40 % | SABIC - Japan Method | break |
Flexural modulus | 23.0 °C | 2.5 GPa Show Supplier Material materials with Flexural modulus of 2.5 GPa | ASTM D 790 |
Flexural strength | 23.0 °C | 98 MPa Show Supplier Material materials with Flexural strength of 98 MPa | ASTM D 790 |
Impact strength, Izod notched | 23.0 °C | 117 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 117 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 117 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 117 J/m | ASTM D 256 |
Tensile strength | 23.0 °C | 63 MPa Show Supplier Material materials with Tensile strength of 63 MPa | SABIC - Japan Method | yield |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 7E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 7E-5 1/K | TMA | -30°C to 30°C | ||
Heat deflection temperature | 105 °C Show Supplier Material materials with Heat deflection temperature of 105 °C | ||||
Heat deflection temperature, 1.80 MPa | 105 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 105 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Flammability | UL Recognized, 94-5VA Flame Class Rating: 2.5mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: 1.5mm UL 94 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 60Hz | 23.0 °C | 2.78 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.78 [-] | ASTM D 150 | 50/60 Hz |
Dissipation factor, 50Hz | 23.0 °C | 3E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 3E-3 [-] | ASTM D 150 | 50/60 Hz |
Sheet resistivity, ROA | 23.0 °C | 1.00E+16 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+16 Ω | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 1.7 g/10min Show Supplier Material materials with Melt mass-flow rate of 1.7 g/10min | ASTM D 1238 | 250°C/10.0 kgf | |
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Photovoltaic Components, Power Manangement, Personal Computing, Washing Machine, Wireless Communications, Document Handling, Displays, Battery Cell, Battery Pack, Auto Electrical, EV Infrastructure, EV/HEV Battery, Enclosures, Energy Management, Enclosure/Housing/Cover, Electronic Components | |
Availability | Europe,Asia,Americas | |
Processing methods | Melt Temperature: 250 to 275.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |