General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.17 g/cm³ Show Supplier Material materials with Density of 1.17 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.32 % Show Supplier Material materials with Moisture absorption of 0.32 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.17 [-] Show Supplier Material materials with Relative density of 1.17 [-] | ASTM D 792 | color |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 3.2 GPa Show Supplier Material materials with Elastic modulus of 3.2 GPa | ASTM D 638 | 5 mm/min |
Elongation | 23.0 °C | 1.9 % Show Supplier Material materials with Elongation of 1.9 % | ISO 527 | yield |
Flexural modulus | 23.0 °C | 3 GPa Show Supplier Material materials with Flexural modulus of 3 GPa | ISO 178 |
Flexural strain | 23.0 °C | 64.1 % Show Supplier Material materials with Flexural strain of 64.1 % | ISO 178 | break, 2 mm/min |
Flexural strength | 23.0 °C | 64 MPa Show Supplier Material materials with Flexural strength of 64 MPa | ISO 178 |
Impact strength, Izod notched | 23.0 °C | 3 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 3 kJ/m² | ISO 180/1A | 80*10*3, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 26 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 26 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched | 23.0 °C | 22 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 22 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 288 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 288 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 36 MPa Show Supplier Material materials with Tensile strength of 36 MPa | ISO 527 | yield |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 8.44E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 8.44E-5 1/K | ASTM E 831 | -30°C to 30°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 9.1E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 9.1E-5 1/K | ASTM E 831 | -30°C to 30°C | ||
Heat deflection temperature | 87 °C Show Supplier Material materials with Heat deflection temperature of 87 °C | ||||
Heat deflection temperature, 1.80 MPa | 87 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 87 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 60 °C Show Supplier Material materials with Relative temperature index, electrical of 60 °C | UL 746B | |||
Relative temperature index, mechanical impact | 60 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 60 °C | UL 746B | |||
Relative temperature index, mechanical strength | 60 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 60 °C | UL 746B | |||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101345219- - <br> UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 1GHz | 23.0 °C | 2.75 [-] Show Supplier Material materials with Dielectric constant, 1GHz of 2.75 [-] | ASTM D 150 |
Dissipation factor, 1GHz | 23.0 °C | 2.4E-3 [-] Show Supplier Material materials with Dissipation factor, 1GHz of 2.4E-3 [-] | ASTM D 150 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Photovoltaic Components, Wireless Communications, Data Transfer, Electronic Components | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |